Lehmann & Voss LUVOCOM® 65-7712/GY PP-copolymer, with carbon fiber and glass fiber, electrically conducting

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Lehmann & Voss & Co.
Trade Name LUVOCOM®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lehmann & Voss LUVOCOM® 65-7712/GY PP-copolymer, with carbon fiber and glass fiber, electrically conducting.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Applications: Office communication.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Information provided by Lehmann & Voss & Co.KG
Physical Properties Metric English Comments
Specific Gravity 1.06 g/cc
1.06 g/cc
ISO 1183
Water Absorption <= 0.30 %
<= 0.30 %
23°C/24h
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
Mechanical Properties Metric English Comments
Tensile Stress 53.0 MPa
7690 psi
Elongation at Yield 1.0 %
1.0 %
1.4 %
1.4 %
flexural
Modulus of Elasticity 8.00 GPa
1160 ksi
Flexural Strength 75.0 MPa
10900 psi
Flexural Modulus 6.00 GPa
870 ksi
Charpy Impact Unnotched 1.40 J/cm²
6.66 ft-lb/in²
edgewise; ISO 179 1eU
Electrical Properties Metric English Comments
Insulation Resistance 100 - 100000 ohm
100 - 100000 ohm
Processing Properties Metric English Comments
Processing Temperature 230 - 260 °C
446 - 500 °F
mass temp
Nozzle Temperature 220 - 250 °C
428 - 482 °F
Zone 1 220 - 250 °C
428 - 482 °F
Zone 2 220 - 250 °C
428 - 482 °F
Zone 3 230 - 260 °C
446 - 500 °F
Mold Temperature 40.0 - 80.0 °C
104 - 176 °F
Drying Temperature 70.0 - 95.0 °C

@Time 7200 - 14400 sec
158 - 203 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Descriptive Properties Value Comments
Color grey
Users viewing this material also viewed the following: