Material Notes:
DescriptionPolyfort® FXP 1227U is a 20% CAC03 filled UV stable copolymer polypropylene product. Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
ASTM D792
Melt Flow 20 g/10 min
20 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 17.0 MPa
2470 psi
ASTM D638
Elongation at Break 10 %
10 %
ASTM D638
Flexural Strength 27.0 MPa
3920 psi
ASTM D790
Flexural Modulus 1.40 GPa
203 ksi
ASTM D790
Izod Impact, Notched 1.90 J/cm
3.56 ft-lb/in
ASTM D256