Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LG Chemical 60HR-G HIPS

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer LG Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical 60HR-G HIPS.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
High flow, Heat resistance, Balanced mechanical properties, Good surface appearance with high gloss, Conforming to FDA CFR 177.1640, Excellent processability, Applications include TV sets, tape recorders, vacuum cleaners, washing machines, and air conditioners
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
ASTM D955
Melt Flow 5.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
5.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 96
96
ASTM D785
Tensile Strength, Yield 26.5 MPa
3840 psi
50 mm/min; ASTM D638
Elongation at Break 70 %
70 %
50 mm/min; ASTM D638
Flexural Yield Strength 43.2 MPa
6270 psi
15 mm/min; ASTM D790
Flexural Modulus 2.00 GPa
290 ksi
15 mm/min; ASTM D790
Izod Impact, Notched 0.830 J/cm

@Thickness 6.35 mm
1.55 ft-lb/in

@Thickness 0.250 in
ASTM D256
1.18 J/cm

@Thickness 3.17 mm
2.21 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C

@Thickness 12.7 mm
176 °F

@Thickness 0.500 in
Unannealed; ASTM D648
Vicat Softening Point 97.0 °C
207 °F
1000 g; ASTM D1525
Flammability, UL94 HB
HB
1/8 in
HB
HB
1/16 in