Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kotec Carbotex K-30FRT12 Polycarbonate, Flame Retardant

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Unreinforced, Flame Retardant
Manufacturer Kotec Corp
Trade Name Carbotex
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Kotec Carbotex K-30FRT12 Polycarbonate, Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Features: Non-brominated & non-chlorined flame retardant, Medium viscosity, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, E & E parts, Safety products, Household applicationsInformation provided by Kotec Corporation
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Water Absorption 0.20 %
<br>@Temperature 23.0 °C,<br> Time 86400 sec
0.20 %
<br>@Temperature 73.4 °F,<br> Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D995
Melt Flow 12 g/10 min
<br>@Load 1.20 kg,<br> Temperature 300 °C
12 g/10 min
<br>@Load 2.65 lb,<br> Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
Tensile Strength at Break 63.0 MPa
9140 psi
ASTM D638
Elongation at Break 120 %
120 %
ASTM D638
Flexural Strength 84.0 MPa
12200 psi
ASTM D790
Flexural Modulus 2.16 GPa
313 ksi
ASTM D790
Izod Impact, Notched 8.30 J/cm
<br>@Temperature 23.0 °C
15.5 ft-lb/in
<br>@Temperature 73.4 °F
V-Notched 1/8&quot;; ASTM D256
Thermal Properties Metric English Comments
Heat Distortion Temperature 133 °C
271 °F
ASTM D648
Flammability, UL94 V-0
<br>@Thickness 3.00 mm
V-0
<br>@Thickness 0.118 in
Optical Properties Metric English Comments
Refractive Index 1.58
1.58
ASTM D542
Haze <= 1.0 %
<br>@Thickness 3.00 mm
<= 1.0 %
<br>@Thickness 0.118 in
ASTM D1003
Transmission, Visible 89 %
<br>@Thickness 3.00 mm
89 %
<br>@Thickness 0.118 in
ASTM D1003
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Constant 2.9
<br>@Frequency 1.00e+6 Hz
2.9
<br>@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 20.0 kV/mm
508 kV/in
ASTM D149
Dissipation Factor 0.0090
<br>@Frequency 1.00e+6 Hz
0.0090
<br>@Frequency 1.00e+6 Hz
ASTM D150
Arc Resistance 110 sec
110 sec
ASTM D495
Copyright © lookpolymers.com All Rights Reserved