| Category | Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Unreinforced |
| Manufacturer | Aclo Compounders |
| Trade Name | Accucomp |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Aclo Accucomp PET PET008L.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.34 g/cc | 0.0484 lb/in³ | ASTM D792 |
| Linear Mold Shrinkage | 0.0030 cm/cm | 0.0030 in/in | MD; ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 113 | 113 | ASTM D785 |
| Tensile Strength at Break | 23.0 MPa | 3340 psi | ASTM D638 |
| Tensile Strength, Yield | 63.0 MPa | 9140 psi | ASTM D638 |
| Elongation at Break | 15 % | 15 % | ASTM D638 |
| Elongation at Yield | 5.0 % | 5.0 % | ASTM D638 |
| Tensile Modulus | 1.826 GPa | 264.9 ksi | ASTM D638 |
| Flexural Strength | 83.01 MPa | 12040 psi | ASTM D790 |
| Flexural Modulus | 2.768 GPa | 401.4 ksi | ASTM D790 |
| Izod Impact, Notched | 0.139 J/cm | 0.260 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 66.1 °C | 151 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 62.8 °C | 145 °F |