Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil 1 Mobilux EP

Category Fluid , Lubricant , Lithium Gellant
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil 1 Mobilux EP.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Mobilux EP 0, 1, 2, 3, and 023 products are a high performance family of five general-purpose industrial greases and two special-duty semi-fluid greases. These lithium hydroxystearate greases are formulated to provide extra protection against wear, rusting and water washout. They are available in NLGI grades ranging from 00 to 3, with base oil viscosities ISO VG 150, 320 and 460. Mobilux EP 0, 1, 2, and 3 greases are recommended for most types of industrial applications including heavy-duty applications where high unit pressures or shock loads are present. These greases provide excellent protection against rust and corrosion and resist water wash-out which makes them particularly suitable for equipment where moist or wet conditions are common. Mobilux EP 0 and 1 are suitable for centralised systems. Mobilux EP 2 and 3 are general-purpose greases. The recommended operating temperature range is from -20ºC to 130ºC but they may be used at higher temperatures if the lubrication frequency is increased accordingly. Mobilux EP 023 is particularly suitable for the lubrication of enclosed gears and bearings in poorly sealed gear cases they can also be used in many other industrial applications where conventional gear oils cannot be retained in gear cases, chain cases, etc. because of leakage due to worn or missing seals. The recommended operating temperature range is -15 to 120ºC for Mobilux EP 023.Mobilux EP 0 and EP 1 provide good low temperature pumpability and are suitable for centralised lubrication systems and other applications where low temperature performance is required.
Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 160 cSt
160 cSt
ASTM D445
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 250 kg
551 lb (mass)
ASTM D2596
Four Ball Wear 0.400 mm
0.0157 in
ASTM D2266
Penetration 325
325
Worked, 25°C; ASTM D217
Timken Test 18100 g
40.0 lb
Thermal Properties Metric English Comments
Dropping Point 190 °C
374 °F
ASTM D2265
Descriptive Properties Value Comments
Color brown
Rust Prevention, Distilled Water pass
ASTM D665A
Soap/Thickener Type lithium
Copyright © lookpolymers.com All Rights Reserved