Material Notes:
Information provided by Kleerdex Company. Kleerdex Company became KYDEX, LLC in 2009.
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
ASTM D792; DIN 53479
Water Absorption 0.30 %
0.30 %
ASTM D570; DIN 53495
Mechanical Properties Metric English Comments
Tensile Strength, Yield 74.5 MPa
10800 psi
ASTM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638; DIN 53455
Modulus of Elasticity 3.30 GPa
479 ksi
ASTM D638; DIN 53452
Flexural Yield Strength 117.7 MPa
17070 psi
ASTM D790; DIN 53455
Flexural Modulus 2.90 GPa
421 ksi
ASTM D790; DIN 53457
Izod Impact, Notched 0.203 J/cm
0.380 ft-lb/in
ASTM D256
Izod Impact, Unnotched (ISO) 2.00 kJ/m²
0.952 ft-lb/in²
JIS K7110
Thermal Properties Metric English Comments
CTE, linear 70.0 µm/m-°C

@Temperature 20.0 °C
38.9 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Specific Heat Capacity 1.47 J/g-°C
0.351 BTU/lb-°F
ASTM C177
Thermal Conductivity 0.210 W/m-K
1.46 BTU-in/hr-ft²-°F
ASTM C177
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F
ASTM D648
Flammability, UL94 HB
HB
Optical Properties Metric English Comments
Refractive Index 1.49
1.49
ASTM D542
Haze 1.36 %
1.36 %
ASTM D1003
Transmission, Visible 86 %
86 %
Transmittance; ASTM D1003
Electrical Properties Metric English Comments
Surface Resistivity per Square 1.00e+6 - 1.00e+8 ohm
1.00e+6 - 1.00e+8 ohm
ASTM D257; DIN 53482
Static Decay 0.0010 sec
0.0010 sec
Electrostatic Discharge; MIL D-81715B
Dielectric Constant 3.5
3.5
ASTM D150; DIN 53483
Descriptive Properties Value Comments
Coating Layer Bond Strength 100/100
JIS D0202
Distinctness of image 98.1
Pencil Hardness H (4H-Cast)