Johnson Matthey JM P40 Soft Solder/Flux

Category Metal , Nonferrous Metal , Solder/Braze Alloy , Tin Alloy
Manufacturer Johnson Matthey
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Johnson Matthey JM P40 Soft Solder/Flux.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General information on the Johnson Matthey soft solder and flux product line: A wide range of Tin/Lead solders suitable for a variety of applications is available from Johnson Matthey. Most materials can be offered as solid wires or as flux cored, to suit the required applications. A wide range of Silver containing solders are suitable for applications where higher strength, increased corrosion resistance or electrical conductivity are required. Federal Specification QQ-S-571 96.5TS ASTM Grade Sn 96BS.EN 29453 Alloy No. 28Information provided by Johnson Matthey.
Thermal Properties Metric English Comments
Melting Point 221 °C
430 °F
Component Elements Properties Metric English Comments
Silver, Ag 4.0 %
4.0 %
Tin, Sn 96 %
96 %