Indium Corp. Indalloy® 7 In-Pb Solder Alloy

Category Metal , Nonferrous Metal , Indium Alloy , Lead Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy® 7 In-Pb Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Indalloy's #7, #10, #150, #204, #205 and #206 comprise a group of lead-indium solders designed to cover the temperature range of 165°C-275°C. All have the minimum gold-leaching characteristics of lead-indium as well as good thermal fatigue properties.Information provided by the manufacturer, Indium Corporation.
Physical Properties Metric English Comments
Density 8.86 g/cc
0.320 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 9.6

@Load 100 kg,
Time 30.0 sec
9.6

@Load 220 lb,
Time 0.00833 hour
Tensile Strength, Ultimate 32.2 MPa
4670 psi
Elongation at Break 55 %
55 %
Shear Strength 18.5 MPa
2680 psi
Shear Bond Holding Strength
Thermal Properties Metric English Comments
CTE, linear 27.0 µm/m-°C

@Temperature 20.0 °C
15.0 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 22.0 W/m-K

@Temperature 85.0 °C
153 BTU-in/hr-ft²-°F

@Temperature 185 °F
Melting Point 184 - 210 °C
363 - 410 °F
Solidus 184 °C
363 °F
Liquidus 210 °C
410 °F
Component Elements Properties Metric English Comments
Indium, In 50 %
50 %
Lead, Pb 50 %
50 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000290 ohm-cm
0.0000290 ohm-cm