Braskem IP2418 LDPE Injection Molding Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Molded
Manufacturer Braskem
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem IP2418 LDPE Injection Molding Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
IP2418 is a low-density polyethylene with good processability and high fluidity, flexibility, and mechanical strength. It does not contain additives. Its applications include injection molding and blends with EVA for foams.
Physical Properties Metric English Comments
Density 0.919 g/cc
0.0332 lb/in³
ASTM-D792
ESCR 10% Igepal® 1.0 hour

@Thickness 2.00 mm,
Temperature 50.0 °C
1.0 hour

@Thickness 0.0787 in,
Temperature 122 °F
0.3 mm notched-plaques; ASTM-D1693
Melt Flow 24 g/10 min

@Load 2.16 kg,
Temperature 190 °C
24 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM-D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 49
49
ASTM-D2240
Tensile Strength at Break 8.00 MPa
1160 psi
ASTM-D638
Tensile Strength, Yield 9.00 MPa
1310 psi
ASTM-D638
Elongation at Break 160 %
160 %
ASTM-D638
Modulus of Rigidity 0.320 GPa
46.4 ksi
ASTM-D747
Flexural Modulus, 1% Secant 300 MPa
43500 psi
ASTM-D790
Thermal Properties Metric English Comments
Vicat Softening Point 82.0 °C

@Load 1.02 kg
180 °F

@Load 2.25 lb
ASTM-D1525
Brittleness Temperature <= -70.0 °C
<= -94.0 °F
ASTM-D746
Descriptive Properties Value Comments
Temperature Profile (°C) 100-150
Blends with EVA
120-180
Injection Molding