TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 80 PHR Mistron Vapor Filler

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer TSE Industries, Inc
Trade Name Millathane®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 80 PHR Mistron Vapor Filler.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear strength, oil and fuel resistance, and ozone resistance. The life expectancy of urethane is often 5 times longer than other elastomers, thus saving material costs and downtime expense. One shortcoming of polyurethanes is loss of physical properties at temperatures over 180°F (82°C). MILLATHANE HT has overcome this weakness.FormulationMillathane HT100.0Zinc Stearate0.5MBTS4.0MBT2.0THANECURE® ZM1.0Sulfur1.5Mistron Vapor80All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 78
78
Tensile Strength, Yield 21.7 MPa
3150 psi
Elongation at Yield 473 %
473 %
100% Modulus 0.009418 GPa
1.366 ksi
200% Modulus 0.01094 GPa
1.587 ksi
300% Modulus 0.01249 GPa
1.812 ksi
Tear Strength 56.2 kN/m
321 pli
Die C
Compression Set 62 %

@Temperature 70.0 °C,
Time 79200 sec
62 %

@Temperature 158 °F,
Time 22.0 hour
Processing Properties Metric English Comments
Cure Time 20.0 min

@Temperature 154 °C
0.333 hour

@Temperature 310 °F
Press cured