Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Asahi Glass AFLAS® 150E TFE/P Fluoroelastomer

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Asahi Glass Company
Trade Name AFLAS®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Asahi Glass AFLAS® 150E TFE/P Fluoroelastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
AFLAS® 100/150 fluoroelastomers are alternating copolymers of tetrafluoroethylene and propylene. They offer 1) excellent heat resistance, 2) exceptional chemical resistance especially to bases and amines, and 3) high electrical resistivity. AFLAS® 100/150 are categorized by ASTM D 1418-01 as class FEPM.Information provided by Asahi Glass Company, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.55 g/cc
1.55 g/cc
ASTM D792
Mooney Viscosity 60

@Temperature 100 °C
60

@Temperature 212 °F
ML1+10
Mechanical Properties Metric English Comments
Hardness, Shore A 71
71
Tensile Strength at Break 14.7 MPa
2130 psi
ASTM D638
Elongation at Break 300 %
300 %
ASTM D638
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -3.00 °C
26.6 °F
Electrical Properties Metric English Comments
Volume Resistivity 3.00e+16 ohm-cm
3.00e+16 ohm-cm
Dielectric Strength 23.0 kV/mm
584 kV/in
ASTM D149
Descriptive Properties Value Comments
Fluorine Content % 57
Users viewing this material also viewed the following: