Material Notes:
Description: Aegis HCA73MP is a lubricated and nucleated low viscosity, nylon 6/6,6 extrusion grade copolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500. It possesses the combination of strength and toughness associated with N6/6,6 as well as excellent heat, chemical, and abrasion resistance. The reduced melt point (385 deg F/196 deg C) of this resin results in lower process melt temperature, lower head pressure, and lower amperage. This translates to higher extrusion rates and thinner nylon layer capabilities. It will also thermoform at lower temperatures and yield higher production rates.Applications:Processed MeatFresh Red MeatPoultryFishCheeseDried FoodChilled Fruit JuicesInformation provided by Honeywell.
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D1505
Water Absorption 0.80 %
0.80 %
Extractable Content
1.4 %
1.4 %
in 24 hours
Moisture Absorption at Equilibrium 2.5 %
2.5 %
at 50% RH
Water Absorption at Saturation 9.0 %
9.0 %
Oxygen Transmission Rate 37.2 cc/m²/day
2.40 cc/100 in²/day
Nitrogen Transmission 7.80 cc-mm/m²-24hr-atm
19.8 cc-mil/100 in²-24hr-atm
cc/m²/day, No thickness given
Carbon Dioxide Transmission 113 cc-mm/m²-24hr-atm
287 cc-mil/100 in²-24hr-atm
cc/m²/day, No thickness given
Viscosity Measurement 3.0
3.0
96% SAV
73
73
FAV; ASTM D789
Maximum Moisture Content 0.080
0.080
Melt Flow 4.5 g/10 min

@Load 1.00 kg,
Temperature 235 °C
4.5 g/10 min

@Load 2.20 lb,
Temperature 455 °F
ASTM D1238
Thermal Properties Metric English Comments
Melting Point 200 °C
392 °F
ASTM D3418
Processing Properties Metric English Comments
Middle Barrel Temperature 225 - 245 °C
437 - 473 °F
Tubular (Blown) Film
225 - 250 °C
437 - 482 °F
Cast Film
Adapter Temperature 243 °C
469 °F
Tubular (Blown) Film
250 °C
482 °F
Cast Film
Die Temperature 240 °C
464 °F
Cast Film
240 °C
464 °F
Tubular (Blown) Film
Melt Temperature 243 °C
469 °F
Tubular (Blown) Film
248 °C
478 °F
Cast Film
Moisture Content 0.080 %
0.080 %