| Category | Metal , Electronic/Magnetic Alloy , Nonferrous Metal , Cobalt Alloy |
| Manufacturer | Goodfellow |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Goodfellow Cobalt/Boron/Silicon/Iron/Molybdenum/Nickel Alloy.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 7.80 g/cc | 0.282 lb/in³ |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Vickers Microhardness | 900 | 900 | kg(f)/mm² |
| Tensile Strength at Break | >= 700 MPa | >= 102000 psi | |
| Tensile Modulus | 63.0 GPa | 9140 ksi |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Crystallization Temperature | 520 °C | 968 °F | |
| Maximum Service Temperature, Air | 80.0 °C | 176 °F |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Boron, B | 12 % | 12 % | |
| Cobalt, Co | 69 % | 69 % | |
| Iron, Fe | 4.0 % | 4.0 % | |
| Molybdenum, Mo | 2.0 % | 2.0 % | |
| Nickel, Ni | 1.0 % | 1.0 % | |
| Silicon, Si | 12 % | 12 % |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 0.000136 ohm-cm | 0.000136 ohm-cm | |
| Magnetic Coercive Force, Hc | 0.010 Oe | 0.010 Oe | |
| Magnetic Saturation Flux Density, Bmax | 7000 Gauss | 7000 Gauss | |
| Curie Temperature | 365 °C | 689 °F |