| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Thickness | 38.1 microns | 1.50 mil | |
| NOVA Chemicals Novapol® LF-0323-B LDPE Film Resin Film Properties. Features: General purpose clarity, good heat sealing latitude, easy processability, good drawdown.Applications: Bakery bags, sandwich bags, zipper lock bags, cast film.Data provide.. |
|||
| Thickness | 38.1 microns | 1.50 mil | Adhesive |
| Dielectric Polymers NT-9511-2 High Tack Tape
(discontinued **) Crosslinked silicone adhesive with polyester film backing.Features: Chemical resistantTemperature resistantGood conformabilityApplications: Splicing of silicone coated paper and film. For applicati.. |
|||
| Thickness | 38.1 microns | 1.50 mil | Adhesive |
| Dielectric Polymers NT-2012-2 Photo Processing Tape
(discontinued **) Crosslinked silicone adhesive with polyester film backing.Features: Chemical resistantTemperature resistantGood conformabilityApplications: Splicing photographic film to leader card during film proc.. |
|||
| Thickness | 38.1 microns | 1.50 mil | |
| ExxonMobil LD 103.MP Industrial Film Resin
(discontinued **) LD 103 resins are homopolymer industrial film resins are used in box and drum liners, industrial packaging, medium duty shrink wrap, construction and agriculture film, and rubber bale wrap.Informati.. |
|||
| Thickness | 38.1 microns | 1.50 mil | |
| NOVA Chemicals Novapol® PF-0118-C Butene LLDPE Film Resin Film Properties. Features: Toughness and strength.Applications: Industrial liners, heavy duty bags.Data provided by the manufacturer. |
|||
| Thickness | 38.1 microns | 1.50 mil | 2:1 BUR |
| LyondellBasell Petrothene® GA501021 Linear Low Density Polyethylene ApplicationsPETROTHENE GA 501series of resins are pelletized linear low density polyethylene for film extrusion applications requiring excellent drawdown and toughness. These resins have excellent .. |
|||
| Thickness | 38.1 microns | 1.50 mil | 2:1 BUR |
| LyondellBasell Petrothene® GA501023 Linear Low Density Polyethylene ApplicationsPETROTHENE GA 501series of resins are pelletized linear low density polyethylene for film extrusion applications requiring excellent drawdown and toughness. These resins have excellent .. |
|||
| Thickness | 38.1 microns | 1.50 mil | |
| Westlake EF796 Low Density Polyethylene Westlake Polyethylene EF796 is a low density formulation suggested for film applications requiring a good balance of properties such as converter film for industrial packaging and general-purpose pa.. |
|||
| Thickness | 38.1 microns | 1.50 mil | ExxonMobil Method |
| ExxonMobil Label-Lyte™ 38LW280 OPP Film Product Description: A super white opaque slip controlled, biaxially oriented polypropylene film, metalized on one side. Designed for use in reel-fed wrap-around applications, where outstanding meta.. |
|||
| Thickness | 38.1 microns | 1.50 mil | |
| ExxonMobil LD 105.BR Very High Clarity Packaging Film Resin Product Description: LD 105 resins are homopolymer packaging film resins designed for applications requiring outstanding clarity with good stiffness. These resins can be processed in either blown or.. |
|||
| Thickness | 38.1 microns | 1.50 mil | |
| ExxonMobil LD 123.LN General Purpose Clarity Film Resin Product Description: LD 123.LN blown film grade offers an excellent balance of optical and strength properties for general purpose clear film applications.Availability: Latin America, North America .. |
|||
| Thickness | 38.1 microns | 1.50 mil | ExxonMobil Method |
| ExxonMobil Metallyte™ 38MW280 OPP Film Product Description: A super white opaque biaxially oriented polypropylene film, metalized on one side. Ideal for single web packaging applications on HFFS in combination with cold seal.Availability.. |
|||
| Thickness | 38.1 microns | 1.50 mil | ExxonMobil Method |
| ExxonMobil Oppalyte™ 38MW247 OPP Film Product Description: A super white opaque biaxially oriented polypropylene film. It is designed for use in cold seal applications where superior optics and graphics are desired.Availability: Africa .. |
|||
| Thickness | 38.1 microns | 1.50 mil | Total; ASTM D3752 |
| 3M 336 Polyester Protective Tape 3M™ Polyester Protective Tape 336 is a thin polyester tape with a low tack adhesive.Information provided by 3M |
|||
| Thickness | 38.1 microns | 1.50 mil | Liner |
| 3M 7000FL Performance Paper Label Material 3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne.. |
|||
| Thickness | 38.1 microns | 1.50 mil | Interleave 1 |
| Arlon 28561R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 1528 FiberglassSide 2: Uncured Silicone RubberInterleave 2: PolyethyleneAppearance: Red silicone gum o.. |
|||
| Thickness | 38.1 microns | 1.50 mil | Interleave 1 |
| Arlon 51571B015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone RubberInterleave 2: Polyethylene This data represents typical.. |
|||
| Thickness | 38.1 microns | 1.50 mil | Polyethylene, Interleave |
| Arlon 57226R020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place o.. |
|||
| Thickness | 38.1 microns | 1.50 mil | Interleave |
| Arlon R35948R015 0.0155" (0.394 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: Polyethylene Side 1, Layer 2: Uncured Silicone RubberSide 1, Layer 1: Cured Silicone Rubber Substrate: Style 7628 Fiberglass Side 2: Cured Silicone RubberThis data re.. |
|||
| Thickness | 38.1 microns | 1.50 mil | Liner |
| 3M FM099 Indoor UL Recognized Matte Silver Polyester Label Product 3M™ Indoor UL Recognized Matte Silver Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize.. |
|||
| Thickness | 38.1 microns | 1.50 mil | Backing; ASTM D3652 |
| 3M 3325 Copper Foil Tape EMI/RFI shielding. UL 510 Recognized.Information provided by 3M |
|||
| Thickness | 38.1 microns | 1.50 mil | Polyethylene Interleave |
| Arlon 30580R010 0.010" (0.254 mm) Uncured/Unsupported Silicone Rubber on a Release Carrier Design/Construction:Side 1: Uncured/Unsupported Silicone Rubber on a Release Carrier Appearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The.. |
|||
| Thickness | 38.1 microns | 1.50 mil | Inner Liner |
| 3M 519YP Sandblast Stencil 3M™ Sandblast Stencil Product 519YP consist of a tan rubber backing; and feature a double liner design for optimum support of center of letters, numbers and designs patterns. The double liner incl.. |
|||
| Thickness | 38.1 - 114 microns | 1.50 - 4.50 mil | Side 2 |
| Arlon 47091R012 0.012" (0.305 mm) Uncured Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured RubberSide 2: Uncured RubberAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The data should not be u.. |
|||
| Thickness | 38.1 microns | 1.50 mil | Backing; ASTM D3652 |
| 3M 8087 Construction Seaming Tape 3M™ Construction Seaming Tape 8087 is designed to seal seams on housewrap and insulated sheathing products. It can also be used to seam polyethylene vapor barrier products as well as to repair hole.. |
|||
| Thickness | 38.1 microns | 1.50 mil | Facestock |
| 3M FA022 Matte Clear Acetate Label Products 3M™ Matte Clear Acetate Label Products offer consistent, high quality film appearance. This film die-cuts easily which helps extend die life in comparison with polyester label stocks. These acetate.. |
|||
| Thickness | 38.1 microns | 1.50 mil | Polyethylene Interleave |
| Arlon 44570B010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Layers Silicone Rubber This data represents typical values for the production material. The data should not be used to write, or in place of, material specificati.. |
|||
| Thickness | 38.1 microns | 1.50 mil | Polyethylene Interleave |
| Arlon 44570R010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Layers Silicone Rubber Appearance: Red silicone gum on fiberglass clothThis data represents typical values for the production material. The data should not be use.. |
|||
| Thickness | 38.1 microns | 1.50 mil | Interleave |
| Arlon 48360X005 0.005" (0.127 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 1080 FiberglassFlame Resistance: Product meets Title 14 CFR 25.856(a) Appendix F, Part VI (amdt. 25-111).. |
|||