Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Escorene™ UL 00226CC Ethylene Vinyl Acetate Copolymer (European Grade)

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer Exxon Chemical
Trade Name Escorene™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escorene™ UL 00226CC Ethylene Vinyl Acetate Copolymer (European Grade).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Description: UL 00226CC is a copolymer of ethylene and vinyl acetate.Processing Conditions: Processing temperature above 230°C (446°F) may cause resin degradation.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Applications: CompoundingHot Melt AdhesivesInjection MoldingProfile ExtrusionTube ExtrusionWire and Cable Compounds Information provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.951 g/cc
0.0344 lb/in³
ExxonMobil method
Vinyl Acetate Content 26 %
26 %
ExxonMobil method
Melt Flow 2.0 g/10 min
2.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 0.689 MPa
>= 100 psi
Molded Properties; ISO 527-2/1A/100
Tensile Modulus 0.0193 GPa
2.80 ksi
Molded Properties; ISO 527-2/1
Thermal Properties Metric English Comments
Melting Point <= 163 °C
<= 325 °F
Peak Melting Point; ExxonMobil method
Vicat Softening Point 46.7 °C
116 °F
ASTM D1525
Descriptive Properties Value Comments
Blending Temperature 230