| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.951 g/cc | 0.0344 lb/in³ | ASTM D1505 |
| Network Polymers NPP 50-0151 Description: High Density Polyethylene (HDPE)Information provided by Network Polymers Inc. |
|||
| Density | 0.951 g/cc | 0.0344 lb/in³ | ASTM D792 |
| North Wood Plastics Polypropylene with 20% Wood Fiber, Extrusion Grade Data provided by North Wood Plastics, Inc. |
|||
| Density | 0.951 g/cc | 0.0344 lb/in³ | ASTM D1505 |
| Chevron Phillips HiD® 9606 HDPE Blown Film and Sheet
(discontinued **) Resin Type: ASTM D 4976 Classification: PE 235, A 54502Applications:General Purpose Films and Sheet, Coextruded Film Structures, Deli and Tissue Films, Sheet Thermoforming Applications with Good Str.. |
|||
| Density | 0.951 g/cc | 0.0344 lb/in³ | ASTM D792-ISO 1183 |
| DuPont Elvax® 205W Ethylene Vinyl Acetate
(discontinued **) DuPont™ Elvax® 205W is an ethylene-vinyl acetate copolymer resin containing an anti-blocking additive for use in industrial applications. This resin is supplied in pellet form and to prevent the p.. |
|||
| Density | 0.951 g/cc | 0.0344 lb/in³ | ASTM D792 |
| Entec Hypel® PEHD32/.951 HDPE
(discontinued **) Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
| Density | 0.951 g/cc | 0.0344 lb/in³ | Exxon Method |
| ExxonMobil Escorene® LD-768 High EVA Film and Compounding Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A low gel 27.5% vinyl acetate copolymer designed for film and compounding applications. The resin provides very low modulus films with high tensile.. |
|||
| Density | 0.951 g/cc | 0.0344 lb/in³ | ASTM D792 |
| NOVA Chemicals Sclair® 2709 HDPE Injection Molding Resin Features: Excellent cold temperature toughness, high stiffness.Applications: Housewares, containers, pails, closures.Data provided by the manufacturer. |
|||
| Density | 0.951 g/cc | 0.0344 lb/in³ | ASTM D792 |
| NOVA Chemicals Sclair® 2710 HDPE Injection Molding Resin Features: Good ESCR, good processability.Applications: Housewares, containers, toys.Data provided by the manufacturer. |
|||
| Density | 0.951 g/cc | 0.0344 lb/in³ | |
| LyondellBasell Lupolen® 5261 ZS HDPE, Blow Molding Grade Relatively high viscosity blow molding grade (similar to Lupolen 5261 Z), but more resistant to stress cracking) for rigid, stackable and highly shock resistant containers for packaging all types of.. |
|||
| Density | 0.951 g/cc | 0.0344 lb/in³ | ASTM D1505 |
| LyondellBasell Plexar® PX2246 Extrudable Tie-Layer Resin - Anhydride Modified HDPE General DescriptionPlexar® tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resin.. |
|||
| Density | 0.951 g/cc | 0.0344 lb/in³ | ASTM D4883 |
| Ineos T50-1000 HDPE Copolymer T50-1000 is a high density polyethylene copolymer. It has a narrow molecular weight distribution and provides injection molded parts with an excellent balance of properties and processing for most g.. |
|||
| Density | 0.951 g/cc | 0.0344 lb/in³ | ASTM D4883 |
| Ineos T50-4400 HDPE Ineos T50-4400 is a high-flow high density polyethylene copolymer intended for injection molding of thin wall containers. This material will allow for cycle time reduction while still imparting rea.. |
|||
| Density | 0.951 - 0.955 g/cc | 0.0344 - 0.0345 lb/in³ | ASTM D792-98 |
| Ipiranga Petrochem GF 5250 HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
| Density | 0.951 g/cc | 0.0344 lb/in³ | compound; ISO 1183 |
| Borealis BorPEX™ HE1878E-C2 High Molecular Weight Polyethylene, Crosslinkable BorPEX™ HE1878E-C2 is a high molecular weight, high density polyethylene specially designed for production of cross linked pipes (PE-X). Applications: BorPEX™ HE1878E-C2 is recommended for the pr.. |
|||
| Density | 0.951 g/cc | 0.0344 lb/in³ | Compound; ISO 1183 |
| Borealis Borstar® HE3494-LS Dark Blue High Density Polyethylene for Drinking Water Pipes Borstar HE3494-LS is a yellow-orange, cadmium free, high density polyethylene compound classified as a MRS 10.0 material (PE100) produced with the advanced Borstar technology. It includes a combina.. |
|||
| Density | 0.951 g/cc | 0.0344 lb/in³ | Compound; ISO 1183 |
| Borealis Borstar® ME3440 Black Medium Density Polyethylene for Pressure Pipes Borstar ME3440 is a black, bimodal medium density polyethylene compound classified as a MRS 8.0 material (PE80), with optimum balance between flexibility and strength, produced with the advanced Bor.. |
|||
| Density | 0.951 g/cc | 0.0344 lb/in³ | ASTM D792-ISO 1183 |
| DuPont Elvax® 220W Ethylene Vinyl Acetate DuPont™ Elvax® 220W is an ethylene-vinyl acetate copolymer resin containing an anti-blocking additive for use in industrial applications. This resin is supplied in pellet form and to prevent the p.. |
|||
| Density | 0.951 g/cc | 0.0344 lb/in³ | ASTM D 792 |
| Total 2285 HDPE Bimodal Film Resin Applications: T-shirt sacks, trash can liners, merchandise bags, multi-wall liner, deli wrapInformation provided provided by Total Petrochemicals. |
|||
| Density | 0.951 g/cc | 0.0344 lb/in³ | ASTM D 792 |
| Total 2287 HDPE Bimodal Film Resin Broad molecular weight distribution. Designed for die build-up sensitive equipmentApplications: T-shirt sacks, trash can liners, merchandise bags, deli wrapInformation provided provided by Total Pe.. |
|||
| Density | 0.951 g/cc | 0.0344 lb/in³ | ExxonMobil Method |
| ExxonMobil Escorene® LD 768.MJ Molding, extrusion and compounding resin Escorene Ultra LD 768.MJ is a high viscosity, 26.2% vinyl acetate copolymer suitable for making very soft, blow molded or extruded articles with very good low temperature toughness. It can also be .. |
|||
| Density | 0.951 g/cc | 0.0344 lb/in³ | ExxonMobil Method |
| ExxonMobil Escorene® UL 7765 Adhesive Application Resin Escorene Ultra UL 7765 is a high viscosity, 26.2% vinyl acetate copolymer that has very good flexibility and low temperature toughness. It has good compatibility with both hydrocarbon and natural t.. |
|||
| Density | 0.951 g/cc | 0.0344 lb/in³ | ExxonMobil method |
| ExxonMobil Escorene™ UL 00226CC Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 00226CC is a copolymer of ethylene and vinyl acetate.Processing Conditions: Processing temperature above 230°C (446°F) may cause resin degradation.Availability: Africa & Mi.. |
|||
| Density | 0.951 g/cc | 0.0344 lb/in³ | ExxonMobil method |
| ExxonMobil Escorene™ UL 04028CC Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 04028CC is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Applications: Hot.. |
|||
| Density | 0.951 g/cc | 0.0344 lb/in³ | ASTM D-792 |
| Bapolene® 5010H High Density Polyethylene This resin is a high molecular weight, high density copolymer polyethylene resin. Product exhibits superior impact strength and ESCR. Resin contains a process stabilizer and complies with FDA 21 C.. |
|||
| Density | 0.951 g/cc | 0.0344 lb/in³ | ExxonMobil method |
| ExxonMobil Escorene™ AD 2528EH2 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: AD 2528EH2 is a copolymer of ethylene and vinyl acetate. Availability: Europe Additive: Antiblock: NoSlip: NoThermal Stabilizer: YesFree Flowing Agent: Yes Applications:Hot Mel.. |
|||
| Density | 0.951 g/cc | 0.0344 lb/in³ | ASTM D4883 |
| Ineos J50-1000-181 HDPE A high density polyethylene copolymer. It has a narrow molecular weight distribution and is intended for the injection molding of screw caps dedicated to the packaging of still water. This resin c.. |
|||
| Density | 0.951 g/cc | 0.0344 lb/in³ | ASTM D4883 |
| Ineos J50-1000-187 HDPE A high density polyethylene copolymer. It has a narrow molecular weight distribution and is intended for the injection molding of screw caps dedicated to the packaging of still water. This resin con.. |
|||
| Density | 0.951 g/cc | 0.0344 lb/in³ | ASTM-D792 |
| Braskem Idealis 500 Compression Molding High Molecular Weight Polyethylene Braskem Idealis 500 is the only high molecular weight polyethylene resin in powder form specially designed for the compression molding process. Its applications range from food handling, cutting boa.. |
|||
| Density | 0.951 g/cc | 0.0344 lb/in³ | ASTM D792 |
| DuPont Elvax® 250 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |
|||
| Density | 0.951 g/cc | 0.0344 lb/in³ | ASTM D792-ISO 1183 |
| DuPont Elvax® 210 Ethylene Vinyl Acetate
(discontinued **) DuPont™ Elvax® 210 is an ethylene-vinyl acetate copolymer resin for use in industrial applications. Applications:Elvax® 210 resins can be used for the following applications: adhesives, sealants,.. |
|||