Premix Thermoplastics PREBLACK PE 700-30

Category Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer Premix Thermoplastics Inc.
Trade Name PREBLACK
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Premix Thermoplastics PREBLACK PE 700-30.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
PREBLACK PE 700-30 is a polyethylene based black masterbatch. PREBLACK PE 700-30 has been developed for the coloring of PE-LD and PE-HD products when maximum UV-resistance and pureness is being required. The moisture absorption and sulphur content of PREBLACK PE 700-30 are very low preventing odor problems. According to BgVV regulations PREBLACK PE 700-30 is approved for use in contact with foodstuffs as long as the content of carbon black in the produced product is less than 2.5%.Information provided by Premix Thermoplastics Inc.
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 300 °C
572 °F
Processing Properties Metric English Comments
Moisture Content <= 0.15 %
<= 0.15 %
When Produced
Shelf Life 12.0 Month
12.0 Month
Normal Storing Conditions
Descriptive Properties Value Comments
Appearance Granule
Carrier PE-LD
Dosing, % 0.5 to 10
Depending on desired blackness and UV-protection
Light Fastness 8-Very Good
Pigmentation, % 30
Special carbon black (p-type)