| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Zone 2 | 185 - 200 °C | 365 - 392 °F | |
| PolyOne OnFlex™ AW 300-02 Thermoplastic Elastomer (TPE) OnFlex™ AW 300-02 is a non-halogen flame retardant material designed for appliance wire applications. New Product. Commercial specifications have not been established.Purge thoroughly before and af.. |
|||
| Zone 2 | 180 - 200 °C | 356 - 392 °F | |
| Lubrizol Advanced Materials PEARLCOAT® Activa D118K Thermoplastic Polyurethane Elastomer PEARLCOAT® Activa D118K is a polycaprolactone copolyester based thermoplastic polyurethane of low hardness, supplied in form of natural pellets. This product gives an inherent “low gloss asp.. |
|||
| Zone 2 | 150 - 200 °C | 302 - 392 °F | |
| Solvay Specialty Polymers Catalyst CAT 10 Polyolefin Catalyst CAT 10 is a high density based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to.. |
|||
| Zone 2 | 150 - 200 °C | 302 - 392 °F | |
| Solvay Specialty Polymers Catalyst CT 0552/09 Polyolefin Catalyst CT 0552/09 is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water.. |
|||
| Zone 2 | 150 - 200 °C | 302 - 392 °F | |
| Solvay Specialty Polymers Catalyst LV/1 Polyolefin Catalyst LV/1 is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water or st.. |
|||
| Zone 2 | 150 - 200 °C | 302 - 392 °F | |
| Solvay Specialty Polymers Catalyst PS/2 Black Polyolefin Catalyst PS/2 is a PE based black catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water.. |
|||
| Zone 2 | 150 - 200 °C | 302 - 392 °F | |
| Solvay Specialty Polymers Catalyst PS/2 Polyolefin Catalyst PS/2 is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that take place by exposure of the pipe to water or steam .. |
|||
| Zone 2 | 150 - 200 °C | 302 - 392 °F | |
| Solvay Specialty Polymers Catalyst PS/2 UV Polyolefin Catalyst PS/2 UV is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water or.. |
|||
| Zone 2 | 150 - 200 °C | 302 - 392 °F | |
| Solvay Specialty Polymers Catalyst PS/4 Polyolefin Catalyst PS/4 is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water or st.. |
|||
| Zone 2 | 150 - 200 °C | 302 - 392 °F | |
| Solvay Specialty Polymers Polidan® PNT 0553/23 Polyethylene, Crosslinked (XLPE) POLIDAN® PNT 0553/23 is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction.Features: Crosslinkable; Good Flexibility; Lo.. |
|||
| Zone 2 | 150 - 200 °C | 302 - 392 °F | |
| Solvay Specialty Polymers Polidan® PNT 0555/06 Polyethylene, Crosslinked (XLPE) POLIDAN® PNT 0555/06 is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes... |
|||
| Zone 2 | 150 - 200 °C | 302 - 392 °F | |
| Solvay Specialty Polymers Polidan® PNT 0856/35 Polyethylene, Crosslinked (XLPE) POLIDAN® PNT 0856/35 is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction.Features: Crosslinkable; Good Flexibility; Lo.. |
|||
| Zone 2 | 150 - 200 °C | 302 - 392 °F | |
| Solvay Specialty Polymers Polidan® S/I 20 Polyethylene, Crosslinked (XLPE) POLIDAN® S/I 20 is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for injection molding.Features: Crossl.. |
|||
| Zone 2 | 150 - 200 °C | 302 - 392 °F | |
| Solvay Specialty Polymers Polidan® T/A Polyethylene, Crosslinked (XLPE) POLIDAN® T/A is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Features.. |
|||
| Zone 2 | 150 - 200 °C | 302 - 392 °F | |
| Solvay Specialty Polymers Polidan® T/A-HF Polyethylene, Crosslinked (XLPE) POLIDAN® T/A-HF is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Featu.. |
|||
| Zone 2 | 150 - 200 °C | 302 - 392 °F | |
| Solvay Specialty Polymers Polidan® T/A-LV Polyethylene, Crosslinked (XLPE) POLIDAN® T/A-LV is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Featu.. |
|||
| Zone 2 | 150 - 200 °C | 302 - 392 °F | |
| Solvay Specialty Polymers Polidan® T/A-LX Polyethylene, Crosslinked (XLPE) POLIDAN® T/A-LX is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Featu.. |
|||
| Zone 2 | 190 - 200 °C | 374 - 392 °F | |
| Lubrizol Estane® X-595A-11 Thermoplastic Polyurethane Type: Estane® X-595A-11 is a Shore 97A, polyester grade thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Extrusion.Available in AsiaInformation Provided by The Lubr.. |
|||
| Zone 2 | 190 - 200 °C | 374 - 392 °F | Injection |
| Lubrizol ESTANE® GP85AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 85AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
| Zone 2 | 190 - 200 °C | 374 - 392 °F | |
| Eurostar Starflam M10004A PP, Flame Retardant, Injection Molding Starflam M10004A is an Unfilled Halogen Free Flame Retardant PP injection Molding ResinInformation provided by Eurostar. |
|||
| Zone 2 | 190 - 200 °C | 374 - 392 °F | |
| Eurostar Starflam M10009A PP, Flame Retardant, Injection Molding Starflam M10009A is an Unfilled Flame Retardant Polypropylene (Homo) Injection Molding ResinInformation provided by Eurostar. |
|||
| Zone 2 | 190 - 200 °C | 374 - 392 °F | |
| Eurostar Starflam MX05036 PP, Flame Retardant, Injection Molding Starflam MX05036 is an Unfilled, Halogen Free Flame Retardant, Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
| Zone 2 | 190 - 200 °C | 374 - 392 °F | |
| Eurostar Starflam MX05075 PP, Flame Retardant, Injection Molding Starflam MX05075 is an Unfilled Halogen Free Flame Retardant PP Injection Molding ResinInformation provided by Eurostar. |
|||
| Zone 2 | 170 - 200 °C | 338 - 392 °F | |
| Eurostar Starglas FF006 HDPE, Glass Fiber Filled Starglas FF004 is a Glass Fiber Reinforced High Density Polyethylene Resin (also known as Starglas PE HE 30V)Information provided by Eurostar. |
|||
| Zone 2 | 190 - 200 °C | 374 - 392 °F | |
| Eurostar Starpylen HU 30E4 ECR PP, Mineral Filled, Injection Molding Starpylen HU 30E4 ECR is a reinforced Polypropylene with a low carbon footprint renewable mineral filler, Injection Molding Resin (also known as HUS30E4ECR)Information provided by Eurostar. |
|||
| Zone 2 | 180 - 200 °C | 356 - 392 °F | |
| Arkema Group OREVAC® 18365-S Grafted Maleic Anhydride Polyethylene OREVAC 18365-S is a grafted maleic anhydride polyethylene used in the manufacturing of multilayer oxygen barrier tube. OREVAC 18365-S is mainly used in multi-layer tube to have good adhesion between.. |
|||
| Zone 2 | 180 - 200 °C | 356 - 392 °F | |
| Arkema Group OREVAC® PPC Grafted Maleic Anhydride Polypropylene OREVAC PPC is a grafted maleic anhydride polypropylene used in the manufacturing of multilayer oxygen barrier tube. OREVAC PPC is mainly used in multi-layer tube to have good adhesion between PP, PA.. |
|||
| Zone 2 | 180 - 200 °C | 356 - 392 °F | Extrusion Molding |
| LG Chemical KEYFLEX BT 1035D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical |
|||