Processing Properties Metric English Comments
Zone 2 190 °C
374 °F
Cylinder
Premix Thermoplastics PRE-ELEC® ESD 6300 Static Dissipative Thermoplastic Compound
PRE-ELEC® ESD 6300 is a static dissipative thermoplastic compound based on high impact polystyrene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD6300 has be..
Zone 2 190 °C
374 °F
Cylinder
Premix Thermoplastics PRE-ELEC® ESD 6610 Static Dissipative Thermoplastic Compound
PRE-ELEC® ESD 6610 is a static dissipative thermoplastic compound based on high impact polystyrene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 6610 has b..
Zone 2 190 - 210 °C
374 - 410 °F
Blow Molding
LG Chemical BM662B ABS, Heat Resistance
Feature: Blow Molding, Heat ResistanceApplication: Automotives Exterior Housing (Spoiler, Bumper Guard etc.)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 31621-07-5Information provided by LG Chemica..
Zone 2 190 - 210 °C
374 - 410 °F
Extrusion Molding
LG Chemical KEYFLEX BT 1040D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
Zone 2 190 - 230 °C
374 - 446 °F
Extrusion Molding
LG Chemical LI931 Extrusion ASA
Description: Low Gloss, Extrusion Application: Industrial Materials (Window Profile, Tile Etc)CAS: 26299-47-8 & 9003-54-7Information provided by LG Chemical
Zone 2 190 - 230 °C
374 - 446 °F
Extrusion Molding
LG Chemical PI641 ABS, High Impact
Feature: Extrusion Molding, General Purpose, High ImpactApplication: Pipe FittingCAS No. 9003-56-9Information provided by LG Chemical
Zone 2 190 - 230 °C
374 - 446 °F
Extrusion Molding
LG Chemical PI642G ABS, General Purpose, High Modulus
Feature: Extrusion Molding, General Purpose, High ModulusApplication: Pipe fittingCAS No. 9003-56-9Information provided by LG Chemical
Zone 2 190 - 230 °C
374 - 446 °F
Extrusion Molding
LG Chemical RS657 ABS, Chemical Resistance to Cyclopentane
Feature: Extrusion Molding, Chemical Resistance to Cyclopentane, Thin ThicknessApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical
Zone 2 190 - 230 °C
374 - 446 °F
Extrusion Molding
LG Chemical RS800M ABS, High Modulus, Chemical Resistance to HCFC
Feature: Extrusion Molding, High Modulus, Chemical Resistance to HCFCApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical
Zone 2 190 - 230 °C
374 - 446 °F
Extrusion Molding
LG Chemical SH610A ABS, High Impact
Feature: Extrusion Molding, General Purpose, High ImpactApplication: Bag, Automobile InteriorCAS No. 9003-56-9Information provided by LG Chemical
Zone 2 190 - 230 °C
374 - 446 °F
Extrusion Molding
LG Chemical SH610S ABS, Excellent Surface, High Impact
Feature: Extrusion Molding, Excellent Surface, High ImpactApplication: Bag, miscellaneousCAS No. 9003-56-9Information provided by LG Chemical
Zone 2 190 - 210 °C
374 - 410 °F
Extrusion Molding
LG Chemical MA221 ABS, High Impact, Low Gloss
Feature: Injection Molding, Extrusion Molding, High Impact, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical
Zone 2 190 °C
374 °F
SK Chemicals SKYTHANE® S195A Polyester Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Zone 2 190 °C
374 °F
SK Chemicals SKYTHANE® S198A Polyester Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Zone 2 190 °C
374 °F
SK Chemicals SKYTHANE® S398A Polyester Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Zone 2 190 °C
374 °F
SK Chemicals SKYTHANE® X595A Polyester Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Zone 2 190 - 200 °C
374 - 392 °F
Injection
Lubrizol ESTANE® GP85AB Ester Based Thermoplastic Polyurethane
Type: Estane® GP 85AB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsInformation provided by Lubrizol.
Zone 2 190 - 200 °C
374 - 392 °F
Injection
Lubrizol ESTANE® GP92AE Ester Based Thermoplastic Polyurethane
Type: Estane® GP 92AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b..
Zone 2 190 - 200 °C
374 - 392 °F
Eurostar Starflam M10004A PP, Flame Retardant, Injection Molding
Starflam M10004A is an Unfilled Halogen Free Flame Retardant PP injection Molding ResinInformation provided by Eurostar.
Zone 2 190 - 200 °C
374 - 392 °F
Eurostar Starflam M10009XP PP, Flame Retardant, Injection Molding
Starflam M10009XP is an Unfilled Flame Retardant Polypropylene (Copolymer) Injection Molding ResinInformation provided by Eurostar.
Zone 2 190 - 200 °C
374 - 392 °F
Eurostar Starpylen HU 30E4 ECR PP, Mineral Filled, Injection Molding
Starpylen HU 30E4 ECR is a reinforced Polypropylene with a low carbon footprint renewable mineral filler, Injection Molding Resin (also known as HUS30E4ECR)Information provided by Eurostar.
Zone 2 190 - 215 °C
374 - 419 °F
Arkema Group OREVAC® 18319 Grafted Maleic Anhydride Polyethylene
OREVAC 18319 is a maleic anhydride grafted polyethylene used in the manufacturing of multi-layer aluminium panels. OREVAC 18319 is mainly used in aluminium panels to have good adhesion performances ..
Zone 2 190 °C
374 °F
Extrusion
Alliance Polymers Viprene™ G80A-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G80A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Zone 2 190 °C
374 °F
Extrusion
Alliance Polymers Viprene™ P75A-22U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ P75A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Zone 2 190 °C
374 °F
Extrusion
Alliance Polymers Viprene™ P80A-22U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ P80A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Zone 2 190 °C
374 °F
Extrusion
Alliance Polymers Viprene™ P85A-22U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ P85A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Zone 2 190 °C
374 °F
Extrusion
Alliance Polymers Zythane™ 5080A Thermoplastic Polyurethane Elastomer
Zythane™ 5080A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Zone 2 190 °C
374 °F
Extrusion
Alliance Polymers Zythane™ 7080A Thermoplastic Polyurethane Elastomer
Zythane™ 7080A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Zone 2 190 - 210 °C
374 - 410 °F
Extrusion Molding