Solvay SIPOMER® COPS-I Sodium 1-Allyloxy-2-Hydroxypropane Sulfonate

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name SIPOMER®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay SIPOMER® COPS-I Sodium 1-Allyloxy-2-Hydroxypropane Sulfonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Co-surfactant monomerChemical Name: SODIUM 1-ALLYLOXY-2-HYDROXYPROPANE SULFONATECAS: 52556-42-0, 7732-18-5, 106-92-3, 106-89-8Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: SIPOMER COPS-I is a Co-polymerizable stabilizer. At low use levels and in combination with conventional surfactants, provides improved latex solubility at low surfactant levels. Improves water resistance and bleach resistance, reduces blocking tendency and reduces loss of adhesion on wetting.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Solids Content 40 - 41 %
40 - 41 %
pH 6.0 - 9.0
6.0 - 9.0
RP-0420
Brookfield Viscosity 60 cP
60 cP
Surface Tension 52.5 dynes/cm
52.5 dynes/cm
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Clear, clean liquid
RP-0064
Color <100
APHA, RP-0134
Composition Active
39-42%
AGE
<0.3%, RP-0146
Conv
0.995
Sodium Bisulfite
<0.1%, RP-0511
Wet Coagulum
0.05%, BOTL
Stability >30 days
Thermal, at 60°C
>5 cycles
F/T
>5 min
Mechanical, Warning Blender