Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ensinger Tecast Vekton™ 6PAG Graphite-Filled Cast Nylon 6 (PA6)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Cast
Manufacturer Ensinger
Trade Name TECAST VEKTON™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger Tecast Vekton™ 6PAG Graphite-Filled Cast Nylon 6 (PA6).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Tecast® 6PAG is a graphite powder-filled with properties similar to MoS2-filled but better suited to wet applications.General Tecast® Cast Nylon Information: Tecast cast nylon, available in a variety of grades, offers a combination of good mechanical properties, excellent bearing and wear characteristics, and the large-size capabilities of the casting process. Its fatigue resistance, noise damping ability, corrosion resistance, and light weight make Tecast ideal for metal replacement applications, such as bearings, gears, sheaves, and sprockets. At one-eight the weight of bronze, Tecast is easier to handle and maintain than metals such as iron, aluminum, brass, and bronze, which it typically replaces in industrial wear applications. Other materials that Tecast commonly replaces because of its superior performance are laminated phenolics, elastomers, and wood. Tecast has excellent wear and abrasion resistance, resulting in extended component life and lower maintenance cost. Its formulations are readily available in rod, plate, and tube. Nonstandard shapes, such as rings, discs, and blocks can be economically produced in small quantities with short lead times. Custom parts can be cast-size or near-net-shape with relatively inexpensive tooling. General Tecast® Application Information: Its unique combination of strength, wear resistance, toughness, machinability, and corrosion resistance make Tecast cast nylon ideal for bearings, thrust washers, bushings, wear pads, sheaves, rollers, gears, sprockets, and wheels. Tecast is commonly used in construction equipment, material handling systems, amusement park rides, pulp and paper processing equipment, steel mills and industrial equipment. Information supplied by Ensinger, Inc.
Physical Properties Metric English Comments
Density 1.14 - 1.15 g/cc
0.0412 - 0.0416 lb/in³
ASTM D792
Water Absorption 0.75 %
0.75 %
at 24 hours; ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100
100
ASTM D785
Tensile Strength, Yield 60.7 MPa
8800 psi
ASTM D638
Elongation at Break 25 %
25 %
ASTM D638
Tensile Modulus 2.41 GPa
350 ksi
ASTM D638
Flexural Strength 86.2 MPa
12500 psi
ASTM D790
Flexural Modulus 2.41 GPa
350 ksi
ASTM D790
Izod Impact, Notched 0.641 J/cm
1.20 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 72.0 µm/m-°C

@Temperature 20.0 °C
40.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Melting Point 220 °C
428 °F
ASTM D2133
Maximum Service Temperature, Air 93.3 °C
200 °F
Long Term; ASTM UL746B
166 °C
330 °F
Intermittent
Electrical Properties Metric English Comments
Dielectric Constant 3.7

@Frequency 60 Hz
3.7

@Frequency 60 Hz
ASTM D150
Dissipation Factor 0.0020

@Frequency 60 Hz
0.0020

@Frequency 60 Hz
ASTM D150