| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.06 g/cc | 0.0383 lb/in³ | ASTM D792 |
| Water Absorption | 0.25 % | 0.25 % | at 24 hours; ASTM D570 |
| Water Absorption at Saturation | 3.0 % | 3.0 % | ASTM D570 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 114 | 114 | ASTM D785 |
| Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
| Elongation at Break | 20 % | 20 % | ASTM D638 |
| Tensile Modulus | 2.07 GPa | 300 ksi | ASTM D638 |
| Flexural Modulus | 1.90 GPa | 275 ksi | ASTM D790 |
| Compressive Strength | 16.5 MPa | 2400 psi | ASTM D695 |
| Izod Impact, Notched | 0.481 J/cm | 0.900 ft-lb/in | ASTM D256 |
| Coefficient of Friction, Static | 0.31 | 0.31 | ASTM D3702 |
| K (wear) Factor | 383 x 10-8 mm³/N-M | 190 x 10-10 in³-min/ft-lb-hr | 40 psi, 50 fpm; ASTM D3702 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
| Specific Heat Capacity | 1.88 J/g-°C | 0.450 BTU/lb-°F | |
| Melting Point | 217 °C | 422 °F | ASTM D2133 |
| Deflection Temperature at 1.8 MPa (264 psi) | 61.1 °C | 142 °F | ASTM D648 |
| Flammability, UL94 | HB @Thickness 0.860 mm |
HB @Thickness 0.0339 in |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | ASTM D257 |
| Dielectric Constant | 3.5 @Frequency 1e+6 Hz |
3.5 @Frequency 1e+6 Hz |
ASTM D150 |
| 4.0 @Frequency 60 Hz |
4.0 @Frequency 60 Hz |
ASTM D150 | |
| Dissipation Factor | 0.020 @Frequency 60 Hz |
0.020 @Frequency 60 Hz |
ASTM D150 |