| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
|
Omni Plastics OmniTech™ PC GR10 Glass Reinforced Polycarbonate
OmniTech™ is a family of non-standard products custom developed for applications with unique functional requirements, including but not limited to: Flame Retardant, Conductive, Wear Resistant, and ..
|
|||
| Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
|
Polymer Resources PC-FR1A-D Polycarbonate, Flame Retardant, Low Flow
Polycarbonate, Flame Retardant, Low FlowFeatures: • High Impact Resistance • High Viscosity • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing co..
|
|||
| Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
|
Polymer Resources PC-FR2A-D Polycarbonate, Flame Retardant, Medium Flow
Polycarbonate, Flame Retardant, Medium FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-i..
|
|||
| Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
|
Polymer Resources PPX-FR5 Modified-PPO, V-0 Flame Retardant
Modified-Polyphenylene Oxide, V-0 Flame Retardant, 225F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-..
|
|||
| Tensile Strength, Yield | 55.2 - 82.7 MPa | 8000 - 12000 psi | ASTM D638 |
|
Alcoa KAMA 2200 Prime Graphic Arts OPS
(discontinued **)
CapabilitiesGauge: .001” to .004” (28 to 101µm)Width: .2” to 80” (50.8 to 2032mm)Core size: 3” and 6” standard cores, 8” availableRoll O.D.: various confiations availableCustom colors and ti..
|
|||
| Tensile Strength, Yield | 55.2 - 82.7 MPa | 8000 - 12000 psi | ASTM D638 |
|
Alcoa KAMA 2600 Envelope Window, Film
(discontinued **)
CapabilitiesGauge: .001” to .004” (28 to 101µm)Width: .2” to 80” (50.8 to 2032mm)Core size: 3” and 6” standard cores, 8” availableRoll O.D.: various confiations availableCustom colors and ti..
|
|||
| Tensile Strength, Yield | 55.2 - 82.7 MPa | 8000 - 12000 psi | ASTM D638 |
|
Alcoa KAMA 2700 OPS Lamination, Film
(discontinued **)
CapabilitiesGauge: .001” to .004” (28 to 101µm)Width: .2” to 80” (50.8 to 2032mm)Core size: 3” and 6” standard cores, 8” availableRoll O.D.: various confiations availableCustom colors and ti..
|
|||
| Tensile Strength, Yield | 55.2 MPa | 8000 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
|
PolyOne Lubri-Tech™ ATH-000/5T Acetal-Homopolymer, PTFE Lubricated
(discontinued **)
Description/Features:PTFE LubricatedInformation provided by PolyOne Corporation.
|
|||
| Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
|
MRC Polymers NAXELLâ„¢ PC429HHI Polycarbonate, Impact Modified, High MFR, EZ Flow
Good Property RetentionHeat and Dimensional StabilityHigh Melt Impact ModifiedMFR can be modified between 10 to 26 g/10minsCan be UV stabilizedGenerally for natural, colorable and can go blackIntern..
|
|||
| Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
|
Techmer ES Electrablend® PA6/6 05012
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: ConductiveInformation provided by TP Composites, Inc.
|
|||
| Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
|
Techmer ES HiFill FR® PA6/6 FR NAT
Availability: North AmericaForms: PelletsFeatures: Flame Retardant UL File Number: E157318Appearance: Natural ColorProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.
|
|||
| Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
|
Techmer ES HiFill® HDPE GF15 50100 15% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightProcessing Method: ExtrusionInformation provided by TP Composites, Inc.
|
|||
| Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D-882 |
|
Saint-Gobain Norton® ECTFE Fluoropolymer Film
Features/Benefits:Outstanding release propertiesPerformance from -200°C (-328°F) to 165°C (330°F)High dielectric strengthExcellent chemical, radiation, weather and abrasion resistanceNon..
|
|||
| Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
|
Techmer ES Plastiblend® PC/PBT IM 1012
Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc.
|
|||
| Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
|
Techmer ES HiFill FR® PC FR SFX-GREEN 1.0
Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Flame RetardantAppearance: GreenInformation provided by TP Composites, Inc.
|
|||
| Tensile Strength, Yield | 55.2 - 131 MPa | 8000 - 19000 psi | 0.2% offset |
|
Eagle Brass 230 Red Brass, Annealed
CDA 230 is known for having an electrical conductivity of 37% IACS, red color, corrosion resistance, excellent formability and moderate strength. Typical uses include costume jewelry, eyelets, faste..
|
|||
| Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
|
Clariant Renol BR7008 Polycarbonate/Polyester Alloy
Data provided by Clariant Masterbatches
|
|||
| Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
|
Clariant Renol PCSP0007 Polycarbonate/Polyester Alloy
Data provided by Clariant Masterbatches
|
|||
| Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
|
Clariant Renol PCSP0016BL-201 Polycarbonate/Polyester Alloy
Data provided by Clariant Masterbatches
|
|||
| Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
|
Ensinger Tecamid® 6/12 Nylon (PA612)
Type 6/12 has lower moisture absorption rates than nylon 6/6, hence superior dimensional stability.Information provided by Ensinger, Inc.
|
|||
| Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
|
Asahi Kasei Thermylene® P1-35FM-1374H 35% Glass/Fiber Reinforced
Information provided by Asahi Thermofil
|
|||
| Tensile Strength, Yield | 55.2 MPa | 8000 psi | ASTM D638 |
|
Asahi Kasei Thermylene® P6-30FG-0877A 30% Glass Fiber Reinforced, UV Stabilized
Information provided by Asahi Thermofil
|
|||
| Tensile Strength, Yield | 55.2 MPa | 8000 psi | |
|
Parylene Coating Services C Poly (P-Xylylene)
Monomer is monochloro para-xylylene. Parylene C is recommended where excellent barrier protection is needed. It can be used up to 125°C where oxygen is present.Parylene is a generic name for poly-..
|
|||
| Tensile Strength, Yield | 55.2 - 82.7 MPa | 8000 - 12000 psi | ASTM D638 |
|
Alcoa KAMA 1120 Prime AntiFog OPS, Sheet
(discontinued **)
CapabilitiesGauge: .005’ to .025” (126 to 635µm)Width: 12” to 62” (305 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone coati..
|
|||
| Tensile Strength, Yield | 55.2 - 82.7 MPa | 8000 - 12000 psi | ASTM D638 |
|
Alcoa KAMA 1100 Prime Clear OPS, Sheet
(discontinued **)
CapabilitiesGauge: .005’ to .025” (126 to 635µm)Width: 12” to 62” (305 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone coati..
|
|||