Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Elektro-Isola Etronit 201M Phenolic, Paper Reinforcement, Dark Brown, Sheets

Category Polymer , Thermoset , Phenolic
Manufacturer Elektro-Isola
Trade Name Etronit
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Elektro-Isola Etronit 201M Phenolic, Paper Reinforcement, Dark Brown, Sheets.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Grade with high mechanical properties but the lowest electrical properties of all Etronit types. Used for mechanical applications.Applications: Dies, topplates and back-up plates for drilling.Information provided by Elektro-Isola
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
24hr/23°C/50% RH; ISO 1183-A; IEC/EN 60893-2 8.1
Water Absorption 3.73 %
3.73 %
24hr/50°C+24hr in water at 23°C,Test Specimen 50x50x3[mm]; ISO 62-1; IEC/EN 60893-2 8.2
Mechanical Properties Metric English Comments
Tensile Strength 130 MPa
<br>@Thickness >=1.50 mm
18900 psi
<br>@Thickness >=0.0591 in
24hr/23°C/50% RH; ISO 527; IEC/EN 60893-2 5.6
Modulus of Elasticity 8.00 GPa
<br>@Thickness >=1.50 mm
1160 ksi
<br>@Thickness >=0.0591 in
24hr/23°C/50% RH; ISO 178; IEC/EN 60893-2 5.2
Flexural Strength 170 MPa
<br>@Thickness >=1.50 mm
24700 psi
<br>@Thickness >=0.0591 in
24hr/23°C/50% RH; ISO 178; IEC/EN 60893-2 5.1
Compressive Strength 310 MPa
<br>@Thickness >=5.00 mm
45000 psi
<br>@Thickness >=0.197 in
24hr/23°C/50% RH; ISO 604; IEC/EN 60893-2 5.3
Shear Strength 35.0 MPa
<br>@Thickness >=5.00 mm
5080 psi
<br>@Thickness >=0.197 in
24hr/23°C/50% RH; IEC/EN 60893-2 5.5
Izod Impact, Notched (ISO) 3.50 kJ/m²
<br>@Thickness >=5.00 mm
1.67 ft-lb/in²
<br>@Thickness >=0.197 in
24hr/23°C/50% RH; ISO 180/2A; IEC/EN 60893-2 5.4.3
Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 120 °C
<br>@Thickness 0.000 mm,<br> Time 7.20e+7 sec
248 °F
<br>@Thickness 0.000 in,<br> Time 20000 hour
IEC 60216; IEC/EN 60893-2 7.1
Electrical Properties Metric English Comments
Insulation Resistance 5.00e+6 ohm
<br>@Thickness >=3.00 mm
5.00e+6 ohm
<br>@Thickness >=0.118 in
24hr/50°C+24h in water at 23°C; IEC 60167; IEC/EN 60893-2 6.3
Dielectric Strength 0.0400 kV/mm
<br>@Thickness >=3.00 mm
1.02 kV/in
<br>@Thickness >=0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60245-1; IEC/EN 60893-2 6.1.3.2
Comparative Tracking Index 100 V
<br>@Thickness 3.00 mm
100 V
<br>@Thickness 0.118 in
IEC 60112; IEC/EN 60893-2 6.4
Copyright © lookpolymers.com All Rights Reserved