Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M 7908 Screen Printable Sheet Polyester Label Material

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 7908 Screen Printable Sheet Polyester Label Material.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials utilize 3M™ Adhesive 350, which is designed to permanently bond to high and low surface energy plastics, textured and contoured surfaces, powder coatings, and slightly oily metals.Information provided by 3M
Physical Properties Metric English Comments
Thickness 45.7 microns
1.80 mil
Adhesive
50.8 microns
2.00 mil
Facestock
170 microns
6.70 mil
Liner
Mechanical Properties Metric English Comments
Peel Strength 0.110 kN/m
0.625 pli
Stainless Steel, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.153 kN/m
0.875 pli
LD Polyethylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.1643 kN/m
0.9375 pli
LD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.29582 kN/m
1.6875 pli
HD Polyethylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.31773 kN/m
1.8125 pli
Polypropylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.3287 kN/m
1.875 pli
LD Polyethylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.33964 kN/m
1.9375 pli
Polypropylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.351 kN/m
2.00 pli
HD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.351 kN/m
2.00 pli
HD Polyethylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.36156 kN/m
2.0625 pli
Polypropylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.3725 kN/m
2.125 pli
Polycarbonate 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.40538 kN/m
2.3125 pli
LD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.4163 kN/m
2.375 pli
HD Polyethylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.438 kN/m
2.50 pli
LD Polyethylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.47112 kN/m
2.6875 pli
LD Polyethylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.51494 kN/m
2.9375 pli
Polypropylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.53686 kN/m
3.0625 pli
Finely Textured Powder Coating, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.5478 kN/m
3.125 pli
HD Polyethylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.5478 kN/m
3.125 pli
Finely Textured Powder Coating, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.570 kN/m
3.25 pli
Finely Textured Powder Coating, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.58068 kN/m
3.3125 pli
LD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.5916 kN/m
3.375 pli
HD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.614 kN/m
3.50 pli
LD Polyethylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.614 kN/m
3.50 pli
HD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.614 kN/m
3.50 pli
Finely Textured Powder Coating, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.6355 kN/m
3.625 pli
HD Polyethylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.64642 kN/m
3.6875 pli
Polycarbonate 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.69024 kN/m
3.9375 pli
Stainless Steel, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.71216 kN/m
4.0625 pli
Polycarbonate 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.7231 kN/m
4.125 pli
Polycarbonate 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.75598 kN/m
4.3125 pli
Glass, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.75598 kN/m
4.3125 pli
Polycarbonate 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.789 kN/m
4.50 pli
Glass, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.79981 kN/m
4.5625 pli
Polypropylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.82172 kN/m
4.6875 pli
Stainless Steel, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.84363 kN/m
4.8125 pli
Glass, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.84363 kN/m
4.8125 pli
Polycarbonate 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.8546 kN/m
4.875 pli
Polypropylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.88746 kN/m
5.0625 pli
Polypropylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.88746 kN/m
5.0625 pli
Stainless Steel, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.90937 kN/m
5.1875 pli
Polypropylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.93128 kN/m
5.3125 pli
Smooth Powder Coating, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.9422 kN/m
5.375 pli
Glass, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.964 kN/m
5.50 pli
Stainless Steel, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.964 kN/m
5.50 pli
Smooth Powder Coating, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.97511 kN/m
5.5625 pli
Glass, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.97511 kN/m
5.5625 pli
Smooth Powder Coating, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.9861 kN/m
5.625 pli
Polycarbonate 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
1.0189 kN/m
5.8125 pli
Glass, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
1.0189 kN/m
5.8125 pli
Smooth Powder Coating, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
1.030 kN/m
5.875 pli
Polycarbonate 180° Peel, Conditioned for 3 days at RT; ASTM D3330
1.05 kN/m
6.00 pli
Stainless Steel, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
1.05 kN/m
6.00 pli
Stainless Steel, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
1.0847 kN/m
6.1875 pli
Glass, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
1.0847 kN/m
6.1875 pli
Stainless Steel, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
1.161 kN/m
6.625 pli
Glass, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 149 °C
300 °F
Service
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Service
10.0 °C
50.0 °F
Application
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Adhesive Type 350 Acrylic
Liner 90# Polyctd.
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved