Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eagle Brass 521 Phosphor Bronzes 8% C, Hard

Category Metal , Nonferrous Metal , Copper Alloy , Bronze
Manufacturer Eagle Brass Company
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Eagle Brass 521 Phosphor Bronzes 8% C, Hard.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical conductivity.Applications include electronic parts, springs, contacts, switch parts and fasteners.Information provided by Eagle Brass Company
Physical Properties Metric English Comments
Density 8.80 g/cc
0.318 lb/in³
Annealed
Mechanical Properties Metric English Comments
Hardness, Rockwell 30T 73 - 80
73 - 80
Thickness > 0.020 Inch
Tensile Strength, Ultimate 586 - 689 MPa
85000 - 100000 psi
Tensile Strength, Yield 538 - 655 MPa
78000 - 95000 psi
0.2% offset
Elongation at Break 12 - 30 %
12 - 30 %
in 2 in.
Tensile Modulus 110 GPa
16000 ksi
Thermal Properties Metric English Comments
CTE, linear 18.2 µm/m-°C

@Temperature 20.0 - 300 °C
10.1 µin/in-°F

@Temperature 68.0 - 572 °F
Thermal Conductivity 62.3 W/m-K
432 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Copper, Cu 91.9 %
91.9 %
Phosphorous, P 0.10 %
0.10 %
Tin, Sn 8.0 %
8.0 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000137 ohm-cm
0.0000137 ohm-cm
Annealed