Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eagle Brass 260 Cartridge Brass, Extra Hard

Category Metal , Nonferrous Metal , Copper Alloy , Brass
Manufacturer Eagle Brass Company
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eagle Brass 260 Cartridge Brass, Extra Hard.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particularly good spring material. The solderability of the alloy is severely impaired by its high zinc content.Information provided by Eagle Brass Company
Physical Properties Metric English Comments
Density 8.53 g/cc
0.308 lb/in³
Annealed
Mechanical Properties Metric English Comments
Hardness, Rockwell 30T 74 - 76
74 - 76
Thickness > 0.020 Inch
Tensile Strength, Ultimate 572 - 634 MPa
83000 - 92000 psi
Tensile Strength, Yield 545 - 600 MPa
79000 - 87000 psi
0.2% offset
Elongation at Break 2.0 - 5.0 %
2.0 - 5.0 %
in 2 in.
Tensile Modulus 110 GPa
16000 ksi
Thermal Properties Metric English Comments
CTE, linear 20.0 µm/m-°C

@Temperature 20.0 - 300 °C
11.1 µin/in-°F

@Temperature 68.0 - 572 °F
Thermal Conductivity 121 W/m-K
840 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Copper, Cu 70 %
70 %
Zinc, Zn 30 %
30 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000636 ohm-cm
0.00000636 ohm-cm
Annealed
Users viewing this material also viewed the following: