| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass Filled, Impact Grade |
| Manufacturer | E-Polymers Co. Ltd. |
| Trade Name | TEKAMID® |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | E-Polymers TEKAMID® TB120G15T Impact Modified, 15% Glass Fiber Reinforced PA6, DAM.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.23 g/cc | 0.0444 lb/in³ | ASTM D792 |
| Linear Mold Shrinkage | 0.0050 cm/cm | 0.0050 in/in |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 110 | 110 | ASTM D786 |
| Tensile Strength, Yield | 100 MPa | 14500 psi | ASTM D638 |
| Elongation at Break | 5.0 % | 5.0 % | ASTM D638 |
| Flexural Yield Strength | 145 MPa | 21000 psi | ASTM D790 |
| Flexural Modulus | 4.40 GPa | 638 ksi | ASTM D790 |
| Izod Impact, Notched | 1.50 J/cm | 2.81 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 50.0 µm/m-°C @Temperature 20.0 °C |
27.8 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
| Melting Point | 220 °C | 428 °F | ASTM D2133 |
| Deflection Temperature at 0.46 MPa (66 psi) | 210 °C | 410 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 200 °C | 392 °F | ASTM D648 |
| Flammability, UL94 | HB | HB |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Arc Resistance | 180 sec | 180 sec | Tungsten electrode; ASTM D495 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 260 - 280 °C | 500 - 536 °F | |
| Mold Temperature | 60.0 - 80.0 °C | 140 - 176 °F |