| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow |
100
µm/m-°C @Temperature -40.0 - 40.0 °C |
55.6
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Geloy XTWE270M ASA+SAN (Asia Pacific)
Excellent weatherability, good flow/aesthetics and good impact.Profile co-extrusion grade over ABS, PVC or other compatible polymers. XTWE270M is available in various colours.This data was supplied..
|
|||
| CTE, linear, Parallel to Flow |
100
µm/m-°C @Temperature 30.0 - 100 °C |
55.6
µin/in-°F @Temperature 86.0 - 212 °F |
|
|
3M Dyneon™ TF 4105 PTFE 25% Glass Fiber Filled
(discontinued **)
Type II PTFE. Applications include valve seats, bearings, seals/gaskets, moldings, piston rings.Data provided by Dyneon.
|
|||
| CTE, linear, Parallel to Flow |
100
µm/m-°C @Temperature 23.0 - 60.0 °C |
55.6
µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Valox® 310SE0 PBT
VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings.
|
|||
| CTE, linear, Parallel to Flow |
100
µm/m-°C @Temperature 23.0 - 60.0 °C |
55.6
µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Valox® 310SE0 PBT (Asia Pacific)
VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings.
|
|||
| CTE, linear, Parallel to Flow |
100
µm/m-°C @Temperature -90.0 - -30.0 °C |
55.6
µin/in-°F @Temperature -130 - -22.0 °F |
3 |
|
Solvay Specialty Polymers Polidan® TUX 100 Polyethylene, Crosslinked (XLPE)
Polidan® TUX 100 is a high density crosslinkable polyethylene compound manufactured according to the Sioplas® process. It has been developed for the production of crosslinked pipes in a wide r..
|
|||
| CTE, linear, Parallel to Flow |
100
µm/m-°C @Temperature 23.0 - 80.0 °C |
55.6
µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Valox® 359 PBT (Europe-Africa-Middle East)
VALOX 359 is an unreinforced, flame retarded, low warpage PBT injection moulding resin.
|
|||
| CTE, linear, Parallel to Flow |
100
µm/m-°C @Temperature 23.0 - 150 °C |
55.6
µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Valox® 359 PBT (Europe-Africa-Middle East)
VALOX 359 is an unreinforced, flame retarded, low warpage PBT injection moulding resin.
|
|||
| CTE, linear, Parallel to Flow |
100
µm/m-°C @Temperature -40.0 - 40.0 °C |
55.6
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Valox® HX312C PBT (Europe-Africa-Middle East)
Unreinforced PBT with release. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant. EtO and stea..
|
|||
| CTE, linear, Parallel to Flow |
100
µm/m-°C @Temperature 23.0 - 80.0 °C |
55.6
µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Valox® HX312C PBT (Europe-Africa-Middle East)
Unreinforced PBT with release. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant. EtO and stea..
|
|||
| CTE, linear, Parallel to Flow |
100
µm/m-°C @Temperature -40.0 - 40.0 °C |
55.6
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Valox® SHF436HR PBT
PBT, Super High Flow, 30% glass reinforced,hydrolytically resistant.
|
|||
| CTE, linear, Parallel to Flow |
100
µm/m-°C @Temperature -40.0 - 40.0 °C |
55.6
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Valox® SHF436HR PBT (Asia Pacific)
PBT, Super High Flow, 30% glass reinforced,hydrolytically resistant.
|
|||
| CTE, linear, Parallel to Flow |
100
µm/m-°C @Temperature -40.0 - 40.0 °C |
55.6
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Valox® SHF436HR PBT (Asia Pacific)
PBT, Super High Flow, 30% glass reinforced,hydrolytically resistant.
|
|||
| CTE, linear, Parallel to Flow |
100
µm/m-°C @Temperature -40.0 - 40.0 °C |
55.6
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Valox® SHF436HR PBT (Europe-Africa-Middle East)
PBT, Super High Flow, 30% glass reinforced,hydrolytically resistant.
|
|||
| CTE, linear, Parallel to Flow |
100
µm/m-°C @Temperature -40.0 - 40.0 °C |
55.6
µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Valox® SHF436HR PBT (Europe-Africa-Middle East)
PBT, Super High Flow, 30% glass reinforced,hydrolytically resistant.
|
|||
| CTE, linear, Parallel to Flow |
100
µm/m-°C @Temperature 23.0 - 60.0 °C |
55.6
µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Xenoy® HX5600HP PBT+PC (Asia Pacific)
Xenoy HX5600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing..
|
|||
| CTE, linear, Parallel to Flow |
100
µm/m-°C @Temperature 23.0 - 60.0 °C |
55.6
µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Xenoy® HX5600HP PBT+PC (Europe-Africa-Middle East)
Xenoy HX5600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing..
|
|||
| CTE, linear, Parallel to Flow |
100
µm/m-°C @Temperature -40.0 - 40.0 °C |
55.6
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Xenoy® HX6600HP PBT+PC
Xenoy HX6600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing..
|
|||
| CTE, linear, Parallel to Flow |
100
µm/m-°C @Temperature -40.0 - 40.0 °C |
55.6
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Xenoy® HX6600HP PBT+PC (Asia Pacific)
Xenoy HX6600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing..
|
|||
| CTE, linear, Parallel to Flow |
100
µm/m-°C @Temperature -40.0 - 40.0 °C |
55.6
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics Xenoy® HX6600HP PBT+PC (Europe-Africa-Middle East)
Xenoy HX6600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing..
|
|||
| CTE, linear, Parallel to Flow |
100
µm/m-°C @Temperature 23.0 - 80.0 °C |
55.6
µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Xenoy® X3108UV PBT+PC (Europe-Africa-Middle East)
Unreinforced, UV-stabilized, flame retardant, impact modified PBT+PC with V0 at 0.8mm thickness. For interior and exterior applications like wall switches and electrical enclosures.This data was sup..
|
|||
| CTE, linear, Parallel to Flow |
100
µm/m-°C @Temperature 23.0 - 60.0 °C |
55.6
µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics NORYL GTX GTX974 PPE+PA (Asia Pacific)
NORYL GTX974 is a material especially designed for in- or on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity for electro-static paintin..
|
|||
| CTE, linear, Parallel to Flow |
100
µm/m-°C @Temperature 23.0 - 60.0 °C |
55.6
µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics NORYL GTX GTX974 PPE+PA (Europe-Africa-Middle East)
NORYL GTX974 is a material especially designed for in- or on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity for electro-static paintin..
|
|||
| CTE, linear, Parallel to Flow |
100
µm/m-°C @Temperature -40.0 - 40.0 °C |
55.6
µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
|
SABIC Innovative Plastics NORYL GTX NX0031 PPE+PA
NORYL GTX* NX0031 resin is a conductive resin specially designed for electrostatic painting and powder coating applications. This material combines high impact, good flow and conductivity. The mate..
|
|||
| CTE, linear, Parallel to Flow |
100
µm/m-°C @Temperature 23.0 - 60.0 °C |
55.6
µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics NORYL GTX NX0031 PPE+PA
NORYL GTX* NX0031 resin is a conductive resin specially designed for electrostatic painting and powder coating applications. This material combines high impact, good flow and conductivity. The mate..
|
|||
| CTE, linear, Parallel to Flow |
100
µm/m-°C @Temperature 23.0 - 60.0 °C |
55.6
µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Noryl HIN120P PPE+HIPS (Europe-Africa-Middle East)
Noryl HIN120P is designed for selected one layer water-based paint systems. Noryl HIN120P has a Vicat B/120 of 120 °C and is targetedThis data was supplied by SABIC-IP for the Europe-Africa-Middl..
|
|||
| CTE, linear, Parallel to Flow |
100
µm/m-°C @Temperature -40.0 - 23.0 °C |
55.6
µin/in-°F @Temperature -40.0 - 73.4 °F |
ISO 11359-1/-2 |
|
DuPont Performance Polymers Delrin® 300PE NC010A Acetal Homopolymer
Delrin® 300PE NC010A is a medium-high viscosity acetal homopolymer, an enhanced version with extremely low VOC emissions. It has improved processing thermal stability, good mechanical properties, a..
|
|||
| CTE, linear, Parallel to Flow |
100
µm/m-°C @Temperature -40.0 - 23.0 °C |
55.6
µin/in-°F @Temperature -40.0 - 73.4 °F |
ISO 11359-1/-2 |
|
DuPont Performance Polymers Delrin® 500PE NC010A Acetal Homopolymer
Delrin® 500PE NC010A is a medium viscosity acetal homopolymer, an enhanced version of Delrin® 500P with extremely low VOC emissions. It has improved processing thermal stability, and good mechanic..
|
|||
| CTE, linear, Parallel to Flow |
100
µm/m-°C @Temperature 55.0 - 160 °C |
55.6
µin/in-°F @Temperature 131 - 320 °F |
DAM; ASTM E 831 |
|
DuPont Performance Polymers Zytel® ST801AHS NC010 Nylon 66
(Unverified Data**)
Zytel® ST801AHS NC010 is a Super Tough, high performance polyamide 66 resin. It offers outstanding molding performance in injection molding applications.Information provided by DuPont
|
|||
| CTE, linear, Parallel to Flow |
100
µm/m-°C @Temperature 55.0 - 160 °C |
55.6
µin/in-°F @Temperature 131 - 320 °F |
DAM; ISO 11359-1/-2 |
|
DuPont Performance Polymers Zytel® ST801AHS NC010 Nylon 66
(Unverified Data**)
Zytel® ST801AHS NC010 is a Super Tough, high performance polyamide 66 resin. It offers outstanding molding performance in injection molding applications.Information provided by DuPont
|
|||
| CTE, linear, Parallel to Flow |
100
µm/m-°C @Temperature -40.0 - 23.0 °C |
55.6
µin/in-°F @Temperature -40.0 - 73.4 °F |
ISO 11359-1/-2 |
|
DuPont Performance Polymers Delrin® 100PE NC010A Acetal Homopolymer
Delrin® 100PE NC010A is a high viscosity acetal homopolymer, an enhanced version of Delrin® 100P with extremely low VOC emissions. It has improved processing thermal stability, good mechanical pro..
|
|||