Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear, Parallel to Flow = 100 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 100 µm/m-°C

@Temperature 30.0 - 100 °C
55.6 µin/in-°F

@Temperature 86.0 - 212 °F
3M Dyneon™ TF 4105 PTFE 25% Glass Fiber Filled  (discontinued **)
Type II PTFE. Applications include valve seats, bearings, seals/gaskets, moldings, piston rings.Data provided by Dyneon.
CTE, linear, Parallel to Flow 100 µm/m-°C

@Temperature 30.0 - 200 °C
55.6 µin/in-°F

@Temperature 86.0 - 392 °F
3M Dyneon™ TF 4215 PTFE 25% Electrocarbon Filled  (discontinued **)
Applications include bearings, seals/gaskets, packings, piston rings.Data provided by Dyneon.
CTE, linear, Parallel to Flow 100 µm/m-°C

@Temperature 23.0 - 60.0 °C
55.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics Valox® 310SE0 PBT
VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings.
CTE, linear, Parallel to Flow 100 µm/m-°C

@Temperature 23.0 - 60.0 °C
55.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics Valox® 310SE0 PBT (Asia Pacific)
VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings.
CTE, linear, Parallel to Flow 100 µm/m-°C

@Temperature -90.0 - -30.0 °C
55.6 µin/in-°F

@Temperature -130 - -22.0 °F
3
Solvay Specialty Polymers Polidan® TUX 100 Polyethylene, Crosslinked (XLPE)
Polidan® TUX 100 is a high density crosslinkable polyethylene compound manufactured according to the Sioplas® process. It has been developed for the production of crosslinked pipes in a wide r..
CTE, linear, Parallel to Flow 100 µm/m-°C

@Temperature -40.0 - 40.0 °C
55.6 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® HX312C PBT (Europe-Africa-Middle East)
Unreinforced PBT with release. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant. EtO and stea..
CTE, linear, Parallel to Flow 100 µm/m-°C

@Temperature 23.0 - 80.0 °C
55.6 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Valox® HX312C PBT (Europe-Africa-Middle East)
Unreinforced PBT with release. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant. EtO and stea..
CTE, linear, Parallel to Flow 100 µm/m-°C

@Temperature -40.0 - 40.0 °C
55.6 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Valox® SHF436HR PBT
PBT, Super High Flow, 30% glass reinforced,hydrolytically resistant.
CTE, linear, Parallel to Flow 100 µm/m-°C

@Temperature -40.0 - 40.0 °C
55.6 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Valox® SHF436HR PBT (Asia Pacific)
PBT, Super High Flow, 30% glass reinforced,hydrolytically resistant.
CTE, linear, Parallel to Flow 100 µm/m-°C

@Temperature -40.0 - 40.0 °C
55.6 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® SHF436HR PBT (Europe-Africa-Middle East)
PBT, Super High Flow, 30% glass reinforced,hydrolytically resistant.
CTE, linear, Parallel to Flow 100 µm/m-°C

@Temperature -40.0 - 40.0 °C
55.6 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Valox® SHF436HR PBT (Europe-Africa-Middle East)
PBT, Super High Flow, 30% glass reinforced,hydrolytically resistant.
CTE, linear, Parallel to Flow 100 µm/m-°C

@Temperature 23.0 - 60.0 °C
55.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics Xenoy® HX5600HP PBT+PC
Xenoy HX5600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing..
CTE, linear, Parallel to Flow 100 µm/m-°C

@Temperature 23.0 - 60.0 °C
55.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics Xenoy® HX5600HP PBT+PC (Europe-Africa-Middle East)
Xenoy HX5600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing..
CTE, linear, Parallel to Flow 100 µm/m-°C

@Temperature -40.0 - 40.0 °C
55.6 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Xenoy® HX6600HP PBT+PC
Xenoy HX6600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing..
CTE, linear, Parallel to Flow 100 µm/m-°C

@Temperature -40.0 - 40.0 °C
55.6 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Xenoy® HX6600HP PBT+PC (Asia Pacific)
Xenoy HX6600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing..
CTE, linear, Parallel to Flow 100 µm/m-°C

@Temperature -40.0 - 40.0 °C
55.6 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Xenoy® HX6600HP PBT+PC (Asia Pacific)
Xenoy HX6600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing..
CTE, linear, Parallel to Flow 100 µm/m-°C

@Temperature 23.0 - 80.0 °C
55.6 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Xenoy® X3108UV PBT+PC (Europe-Africa-Middle East)
Unreinforced, UV-stabilized, flame retardant, impact modified PBT+PC with V0 at 0.8mm thickness. For interior and exterior applications like wall switches and electrical enclosures.This data was sup..
CTE, linear, Parallel to Flow 100 µm/m-°C

@Temperature -40.0 - 40.0 °C
55.6 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Noryl GTX GTX9200 PPE+PS+PA66 (Asia Pacific)
High Flow GTX for Automotive applicationsThis data was supplied by SABIC-IP for the Asia Pacific region.
CTE, linear, Parallel to Flow 100 µm/m-°C

@Temperature -40.0 - 40.0 °C
55.6 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Noryl GTX GTX9200 PPE+PS+PA66 (Europe-Africa-Middle East)
High Flow GTX for Automotive applicationsThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
CTE, linear, Parallel to Flow 100 µm/m-°C

@Temperature 23.0 - 60.0 °C
55.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics NORYL GTX GTX974 PPE+PA
NORYL GTX974 is a material especially designed for in- or on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity for electro-static paintin..
CTE, linear, Parallel to Flow 100 µm/m-°C

@Temperature 23.0 - 60.0 °C
55.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics NORYL GTX GTX974 PPE+PA (Europe-Africa-Middle East)
NORYL GTX974 is a material especially designed for in- or on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity for electro-static paintin..
CTE, linear, Parallel to Flow 100 µm/m-°C

@Temperature -40.0 - 40.0 °C
55.6 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL GTX NX0031 PPE+PA
NORYL GTX* NX0031 resin is a conductive resin specially designed for electrostatic painting and powder coating applications. This material combines high impact, good flow and conductivity. The mate..
CTE, linear, Parallel to Flow 100 µm/m-°C

@Temperature 23.0 - 60.0 °C
55.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics NORYL GTX NX0031 PPE+PA
NORYL GTX* NX0031 resin is a conductive resin specially designed for electrostatic painting and powder coating applications. This material combines high impact, good flow and conductivity. The mate..
CTE, linear, Parallel to Flow 100 µm/m-°C

@Temperature 23.0 - 60.0 °C
55.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics Noryl HIN120P PPE+HIPS (Europe-Africa-Middle East)
Noryl HIN120P is designed for selected one layer water-based paint systems. Noryl HIN120P has a Vicat B/120 of 120 °C and is targetedThis data was supplied by SABIC-IP for the Europe-Africa-Middl..
CTE, linear, Parallel to Flow 100 µm/m-°C

@Temperature 23.0 - 80.0 °C
55.6 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Xenoy® X3108UV PBT+PC (Asia Pacific)
Unreinforced, UV-stabilized, flame retardant, impact modified PBT+PC with V0 at 0.8mm thickness. For interior and exterior applications like wall switches and electrical enclosures.This data was sup..
CTE, linear, Parallel to Flow 100 µm/m-°C

@Temperature -40.0 - 23.0 °C
55.6 µin/in-°F

@Temperature -40.0 - 73.4 °F
ISO 11359-1/-2
DuPont Performance Polymers Delrin® 300PE NC010A Acetal Homopolymer
Delrin® 300PE NC010A is a medium-high viscosity acetal homopolymer, an enhanced version with extremely low VOC emissions. It has improved processing thermal stability, good mechanical properties, a..
CTE, linear, Parallel to Flow 100 µm/m-°C

@Temperature -40.0 - 23.0 °C
55.6 µin/in-°F

@Temperature -40.0 - 73.4 °F
ISO 11359-1/-2
DuPont Performance Polymers Delrin® 500PE NC010A Acetal Homopolymer
Delrin® 500PE NC010A is a medium viscosity acetal homopolymer, an enhanced version of Delrin® 500P with extremely low VOC emissions. It has improved processing thermal stability, and good mechanic..
CTE, linear, Parallel to Flow 100 µm/m-°C

@Temperature 55.0 - 160 °C
55.6 µin/in-°F

@Temperature 131 - 320 °F
DAM; ASTM E 831
DuPont Performance Polymers Zytel® ST801AHS NC010 Nylon 66  (Unverified Data**)
Zytel® ST801AHS NC010 is a Super Tough, high performance polyamide 66 resin. It offers outstanding molding performance in injection molding applications.Information provided by DuPont
CTE, linear, Parallel to Flow 100 µm/m-°C

@Temperature 55.0 - 160 °C
55.6 µin/in-°F

@Temperature 131 - 320 °F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® ST801AHS NC010 Nylon 66  (Unverified Data**)
Zytel® ST801AHS NC010 is a Super Tough, high performance polyamide 66 resin. It offers outstanding molding performance in injection molding applications.Information provided by DuPont
CTE, linear, Parallel to Flow 100 µm/m-°C

@Temperature -40.0 - 23.0 °C
55.6 µin/in-°F

@Temperature -40.0 - 73.4 °F
ISO 11359-1/-2
DuPont Performance Polymers Delrin® 100PE NC010A Acetal Homopolymer
Delrin® 100PE NC010A is a high viscosity acetal homopolymer, an enhanced version of Delrin® 100P with extremely low VOC emissions. It has improved processing thermal stability, good mechanical pro..