Shakespeare LMX-3 Easy Casting Nylon Copolymer Fishing Line, 20 lb

Category Polymer , Thermoplastic , Nylon
Manufacturer Shakespeare Company
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shakespeare LMX-3 Easy Casting Nylon Copolymer Fishing Line, 20 lb.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Soft, limp and low line memory. Excellent cold casting properties. Especially designed for reels with tight arbors (example: micro spin casting reels)Information provided by Shakespeare Company.
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 634 MPa
>= 92000 psi
23.4 lb. Minimum Tensile Load 0.018 in. Diameter
Elongation at Break 25 - 35 %
25 - 35 %