| Category | Polymer , Adhesive , Thermoset , Silicone , Silicone, RTV, Adhesive/Sealant Grade |
| Manufacturer | Dow Corning |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Dow Corning 739 PLASTIC ADHESIVE.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.52 g/cc @Temperature 25.0 °C |
1.52 g/cc @Temperature 77.0 °F |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 37 | 37 | |
| Tensile Strength, Ultimate | 1.55 MPa | 225 psi | |
| Elongation at Break | 640 % | 640 % | |
| Shear Strength | 1.38 MPa | 200 psi | |
| Tear Strength | 6.49 kN/m | 37.0 pli | |
| Peel Strength | 3.51 kN/m | 20.0 pli |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 200 °C | 392 °F | |
| Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | |
| Flammability, UL94 | HB | HB |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 6.10e+14 ohm-cm | 6.10e+14 ohm-cm | |
| Dielectric Constant | 3.7 @Frequency 100 Hz |
3.7 @Frequency 100 Hz |
|
| 3.7 @Frequency 100000 Hz |
3.7 @Frequency 100000 Hz |
||
| Dissipation Factor | 0.0020 @Frequency 100 Hz |
0.0020 @Frequency 100 Hz |
|
| <= 0.0020 @Frequency 100000 Hz |
<= 0.0020 @Frequency 100000 Hz |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Cure Time | 1440 min @Temperature 22.0 °C |
24.0 hour @Temperature 71.6 °F |
|
| Shelf Life | 15.0 Month | 15.0 Month |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | Black | |
| white | ||
| Flowable | no | |
| Hydrophobic | yes | |
| Water Resistant | yes |