3M FM05540K MC Polyester Label Product

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M FM05540K MC Polyester Label Product.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
3M™ MC Polyester Label Products are white durable, high performance micro-cavitated polyester materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ Adhesive F2201, which offers high initial tack, good clarity and adhesion when applied at low temperatures and excellent processing characteristics.Information provided by 3M
Physical Properties Metric English Comments
Thickness 50.8 microns
2.00 mil
Facestock
73.7 microns
2.90 mil
Liner
Mechanical Properties Metric English Comments
Peel Strength 0.351 kN/m
2.00 pli
180° Peel, 12"/min., 1" wide sample; TLMI Method
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 49.0 °C
120 °F
Application
150 °C
302 °F
Service
Minimum Service Temperature, Air -29.0 °C
-20.2 °F
Service
-18.0 °C
-0.400 °F
Application
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Adhesive Type F2201 Freezer 30
Liner 83# Laser