PlastiComp Complet® LCF40-PPA Polyphthalamide, 40% Long Carbon Fiber Reinforced

Category Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), Carbon Fiber Filled
Manufacturer PlastiComp
Trade Name Complēt®
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF PlastiComp Complet® LCF40-PPA Polyphthalamide, 40% Long Carbon Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyphthalamide with 40% long carbon fiber reinforcementInformation provided by PlastiComp, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.37 g/cc
1.37 g/cc
ASTM D-792
Filler Content 40 %
40 %
Long Carbon Fiber
Mechanical Properties Metric English Comments
Tensile Strength 314 MPa
45500 psi
ASTM D-638
Elongation at Break <= 1.0 %
<= 1.0 %
ASTM D-638
Tensile Modulus 37.931 GPa
5501.4 ksi
ASTM D-638
Flexural Strength 476 MPa
69000 psi
ASTM D-790
Flexural Modulus 28.276 GPa
4101.1 ksi
ASTM D-790
Izod Impact, Notched 2.14 J/cm
4.01 ft-lb/in
ASTM D-256
Izod Impact, Unnotched 9.08 J/cm
17.0 ft-lb/in
ASTM D-4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 277 °C
531 °F
ASTM D-648