Material Notes:
Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many specific potting and encapsulating applications such as modules, strain-sensitive components, transformers, and coils. All 2500 series systems exhibit excellent performance when exposed to adverse environments and temperature ranges between -55°C and +130°C.Cytec (Conap) EN-2534 Potting and Encapsulation AdhesivePasses Thermal Shock Test (10 Cycles, -65°C to 130°C)Non-Nutrient Fungus Resistance (MIL-STD-810B)Mix Ratio: 20/100 (by Weight)
Physical Properties Metric English Comments
Density 1.45 g/cc
0.0524 lb/in³
Cured
Water Absorption 0.15 %
0.15 %
24 hours
Water Absorption at Saturation 0.0045 %
0.0045 %
30 Days
Viscosity 2200 cP
<br>@Temperature 25.0 °C
2200 cP
<br>@Temperature 77.0 °F
Linear Mold Shrinkage 0.0065 cm/cm
0.0065 in/in
Mechanical Properties Metric English Comments
Hardness, Shore D 50 - 55
50 - 55
Tensile Strength, Ultimate 13.6 MPa
1970 psi
Elongation at Break 60 %
60 %
Thermal Properties Metric English Comments
CTE, linear 150 µm/m-°C
<br>@Temperature 20.0 °C
83.3 µin/in-°F
<br>@Temperature 68.0 °F
Thermal Conductivity 0.188 W/m-K
1.30 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 130 °C
266 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Electrical Properties Metric English Comments
Volume Resistivity <= 3.40e+13 ohm-cm
<= 3.40e+13 ohm-cm
Surface Resistance 1.50e+13 ohm
1.50e+13 ohm
Dielectric Constant 4.1
<br>@Frequency 1000 Hz
4.1
<br>@Frequency 1000 Hz
Dielectric Strength 23.0 kV/mm
<br>@Thickness 1.59 mm
584 kV/in
<br>@Thickness 0.0625 in
Dissipation Factor 0.049
<br>@Frequency 1000 Hz
0.049
<br>@Frequency 1000 Hz
Arc Resistance >= 120 sec
>= 120 sec
Processing Properties Metric English Comments
Cure Time 120 min
<br>@Temperature 100 °C
2.00 hour
<br>@Temperature 212 °F
960 min
<br>@Temperature 80.0 °C
16.0 hour
<br>@Temperature 176 °F
10080 min
<br>@Temperature 25.0 °C
168.0 hour
<br>@Temperature 77.0 °F
Pot Life 15.0 - 20.0 min
<br>@Temperature 25.0 °C
15.0 - 20.0 min
<br>@Temperature 77.0 °F
1 lbm
Descriptive Properties Value Comments
Color Black