Material Notes:
Nonoriented electrical steels are silicon steels in which magnetic properties are practically the same in any direction of magnetism in the plane of the material. Standard grades from M-15 to M-47 are available with the advantages of special DI-MAX® processing that enhance the magnetic properties. DI-MAX grades have superior permeability at high inductions, low average core loss and good gauge uniformity. In addition, cold finishing plus strip annealing produce a smooth surface and reduce buckles and waves, resulting in excellent flatness and a high stacking factor. AK Steel Nonoriented Electrical Steels are available both Fully Processed and Semi-Processed, depending on grade. Properties of Fully Processed material are developed completely by AK Steel. These materials are ready for use without any additional processing required. However, a low-temperature heat treatment may be employed by the user to eliminate stresses introduced by fabrication of the material into cores. AK Steel Fully Processed Nonoriented Electrical Steels meet all the requirements of ASTM Specification A 677. Semi-Processed steels are finished to final thickness and physical form by AK Steel, but are not fully annealed to develop final magnetic quality. With these materials, achievement of magnetic properties becomes the responsibility of the user. AK Steel Semi-Processed Nonoriented Electrical Steels meet all requirements of ASTM A 683. DI-MAX M-47 is Fully Processed and Semi-Processed Applications for M-47: Small Motors and Generators (
Physical Properties Metric English Comments
Density 7.75 g/cc
0.280 lb/in³
Semi-Processed and Fully Processed
Mechanical Properties Metric English Comments
Hardness, Rockwell B 61
61
Fully Processed
62
62
Semi-Processed
Tensile Strength, Ultimate 427 MPa
62000 psi
Fully Processed
462 MPa
67000 psi
Semi-Processed
Tensile Strength, Yield 269 MPa
39000 psi
Fully Processed
331 MPa
48000 psi
Semi-Processed
Elongation at Break 33 %
33 %
in 2", Semi-Processed
34 %
34 %
in 2", Fully Processed
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000370 ohm-cm
0.0000370 ohm-cm
Fully Processed and Semi-Processed
Magnetic Properties Metric English Comments
Core Loss 3.64 W/kg

@Magnetic Field 1.50 T,
Frequency 60.0 Hz
1.65 W/lb

@Magnetic Field 1.50 T,
Frequency 60.0 Hz
0.0185" (26 gauge), Semi-Processed; ASTM A677
4.63 W/kg

@Magnetic Field 1.50 T,
Frequency 60.0 Hz
2.10 W/lb

@Magnetic Field 1.50 T,
Frequency 60.0 Hz
0.025" (24 gauge), Semi-Processed; ASTM A677
6.17 W/kg

@Magnetic Field 1.50 T,
Frequency 60.0 Hz
2.80 W/lb

@Magnetic Field 1.50 T,
Frequency 60.0 Hz
0.0185" (26 gauge), Fully Processed; ASTM A677
7.05 W/kg

@Magnetic Field 1.50 T,
Frequency 60.0 Hz
3.20 W/lb

@Magnetic Field 1.50 T,
Frequency 60.0 Hz
0.025" (24 gauge), Fully Processed; ASTM A677
Descriptive Properties Value Comments
Coercive Force (Oe) 0.28
B<sub>max</sub> =10kG, Semi-Processed
0.57
B<sub>max</sub> =10kG, Fully Processed
Hysteresis loss (J/lb/cycle) 0.0050
B<sub>max</sub> =10kG, Semi-Processed
0.0094
B<sub>max</sub> =10kG, Fully Processed
Maximum Permeability 16300
Semi-Processed
6800
Fully Processed
Saturation Induction Kilogausses 20.8
Fully Processed
20.8
Semi-Processed
Users viewing this material also viewed the following: