Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Covestro Makrolon® 2405 Polycarbonate, Injection Grade

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Unreinforced, Flame Retardant
Manufacturer Covestro
Trade Name Makrolon®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Covestro Makrolon® 2405 Polycarbonate, Injection Grade.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Very easy flowing injection molding grade with easy mold release, Makrolon grade 2458 for food contact applications.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
Water Absorption 0.35 %
0.35 %
Saturation in water
Moisture Absorption at Equilibrium 0.15 %
0.15 %
Equilibrium at 50% RH
Water Absorption at Saturation 0.35 %
0.35 %
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D955
Melt Flow 19 g/10 min
<br>@Load 1.20 kg,<br> Temperature 300 °C
19 g/10 min
<br>@Load 2.65 lb,<br> Temperature 572 °F
Mechanical Properties Metric English Comments
Hardness, Rockwell M 75
75
ASTM D785
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength, Ultimate 69.0 MPa
10000 psi
ASTM D638
Tensile Strength, Yield 63.0 MPa
9140 psi
Elongation at Break 120 %
120 %
ASTM D638
Elongation at Yield 6.0 %
6.0 %
Tensile Modulus 2.30 GPa
334 ksi
Flexural Yield Strength 83.0 MPa
12000 psi
at 5% strain; ASTM D790
Flexural Modulus 2.30 GPa
334 ksi
ASTM D790
Izod Impact, Notched 7.50 J/cm
<br>@Thickness 3.20 mm
14.1 ft-lb/in
<br>@Thickness 0.126 in
ASTM D256
Charpy Impact Unnotched NB
NB
Tensile Creep Modulus, 1 hour 2200 MPa
319000 psi
Tensile Creep Modulus, 1000 hours 1900 MPa
276000 psi
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
<br>@Temperature 20.0 °C
38.9 µin/in-°F
<br>@Temperature 68.0 °F
CTE, linear, Transverse to Flow 70.0 µm/m-°C
<br>@Temperature 20.0 °C
38.9 µin/in-°F
<br>@Temperature 68.0 °F
Specific Heat Capacity 1.17 J/g-°C
0.280 BTU/lb-°F
ASTM D2766
Thermal Conductivity 0.200 W/m-K
1.39 BTU-in/hr-ft²-°F
ASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 137 °C
279 °F
Deflection Temperature at 1.8 MPa (264 psi) 124 °C
255 °F
Vicat Softening Point 144 °C
291 °F
Glass Transition Temp, Tg 148 °C
298 °F
UL RTI, Electrical 125 °C
257 °F
UL RTI, Mechanical with Impact 115 °C
239 °F
UL RTI, Mechanical without Impact 125 °C
257 °F
Flammability, UL94 V-2
<br>@Thickness 2.60 mm
V-2
<br>@Thickness 0.102 in
V-2
<br>@Thickness 1.60 mm
V-2
<br>@Thickness 0.0630 in
Oxygen Index 26 %
26 %
Optical Properties Metric English Comments
Refractive Index 1.584
1.584
Haze 1.0 %
<br>@Thickness 3.17 mm
1.0 %
<br>@Thickness 0.125 in
ASTM D1003
Transmission, Visible 88 %
<br>@Thickness 3.20 mm
88 %
<br>@Thickness 0.126 in
ASTM D1003
Electrical Properties Metric English Comments
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
Surface Resistance 1.00e+15 ohm
1.00e+15 ohm
Dielectric Constant 2.9
<br>@Frequency 1e+6 Hz
2.9
<br>@Frequency 1e+6 Hz
3.0
<br>@Frequency 100 Hz
3.0
<br>@Frequency 100 Hz
Dielectric Strength 30.0 kV/mm
762 kV/in
Dissipation Factor 0.0010
<br>@Frequency 100 Hz
0.0010
<br>@Frequency 100 Hz
0.010
<br>@Frequency 1e+6 Hz
0.010
<br>@Frequency 1e+6 Hz
Arc Resistance 120 sec
120 sec
Tungsten Electrodes; ASTM D495
Comparative Tracking Index 275 V
275 V
Hot Wire Ignition, HWI 30 - 60 sec
<br>@Thickness 1.50 mm
30 - 60 sec
<br>@Thickness 0.0591 in
UL PLC 2 (30-60 s)
30 - 60 sec
<br>@Thickness 3.00 mm
30 - 60 sec
<br>@Thickness 0.118 in
UL PLC 2 (30-60 s)
High Amp Arc Ignition, HAI 60 - 120 arcs
<br>@Thickness 3.00 mm
60 - 120 arcs
<br>@Thickness 0.118 in
UL PLC 1 (60-120 arcs)
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/min
<br>@Thickness 3.00 mm
0.000 - 0.394 in/min
<br>@Thickness 0.118 in
UL PLC 0 (0-10 mm/min)
Copyright © lookpolymers.com All Rights Reserved