| Category | Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) |
| Manufacturer | Chevron Phillips Chemical Company LP |
| Trade Name | Xtel® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Chevron Phillips Xtel® XE4050BL Polyphenylene Sulfide Alloy.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.70 g/cc | 0.0614 lb/in³ | ISO 1183A |
| Water Absorption | 0.030 % | 0.030 % | ASTM D-570 |
| Linear Mold Shrinkage, Flow | 0.0020 cm/cm | 0.0020 in/in | |
| Linear Mold Shrinkage, Transverse | 0.0040 cm/cm | 0.0040 in/in |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 130 MPa | 18900 psi | ISO 527 |
| Elongation at Yield | 1.7 % | 1.7 % | ISO 527 |
| Flexural Strength | 190 MPa | 27600 psi | ISO 178 |
| Flexural Modulus | 11.0 GPa | 1600 ksi | ISO 178 |
| Compressive Strength | 195 MPa | 28300 psi | ISO 604 |
| Izod Impact, Notched (ISO) | 7.00 kJ/m² | 3.33 ft-lb/in² | ISO 180A |
| Izod Impact, Unnotched (ISO) | 35.0 kJ/m² | 16.7 ft-lb/in² | ISO 180A |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 10.0 µm/m-°C <br>@Temperature 100 - 200 °C |
5.56 µin/in-°F <br>@Temperature 212 - 392 °F |
Axial; ISO 11359-2 |
| 20.0 µm/m-°C <br>@Temperature -50.0 - 50.0 °C |
11.1 µin/in-°F <br>@Temperature -58.0 - 122 °F |
Axial; ISO 11359-2 | |
| CTE, linear, Transverse to Flow | 50.0 µm/m-°C <br>@Temperature -50.0 - 50.0 °C |
27.8 µin/in-°F <br>@Temperature -58.0 - 122 °F |
ISO 11359-2 |
| 100 µm/m-°C <br>@Temperature 100 - 200 °C |
55.6 µin/in-°F <br>@Temperature 212 - 392 °F |
ISO 11359-2 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 255 °C | 491 °F | ISO 75 |
| Flammability, UL94 | V-0 | V-0 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | ASTM D-257 |
| Dielectric Constant | 4.0 <br>@Frequency 1e+6 Hz |
4.0 <br>@Frequency 1e+6 Hz |
ASTM D-150 |
| 4.1 <br>@Frequency 1000 Hz |
4.1 <br>@Frequency 1000 Hz |
ASTM D-150 | |
| Dielectric Strength | 20.0 kV/mm | 508 kV/in | ASTM D-149 |
| Dissipation Factor | 0.0030 <br>@Frequency 1000 Hz |
0.0030 <br>@Frequency 1000 Hz |
ASTM D-150 |
| 0.0090 <br>@Frequency 1e+6 Hz |
0.0090 <br>@Frequency 1e+6 Hz |
ASTM D-150 | |
| Arc Resistance | 120 sec | 120 sec | ASTM D-495 |
| Comparative Tracking Index | 150 V | 150 V | UL 746A |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 315 - 345 °C | 599 - 653 °F | |
| Mold Temperature | 135 °C | 275 °F |