Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Cheng Yu Plastic N6GV25 Flame Retardant Nylon 6, 25% Glass Filled

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled
Manufacturer Cheng Yu Plastic Company Limited (formerly Luen Cheong Hong)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cheng Yu Plastic N6GV25 Flame Retardant Nylon 6, 25% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.25 g/cc
1.25 g/cc
ASTM D792
Water Absorption 0.15 %
0.15 %
ASTM D570
Linear Mold Shrinkage 0.0080 - 0.015 cm/cm
0.0080 - 0.015 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 95
95
ASTM D785
Tensile Strength, Yield 154 MPa
22300 psi
ASTM D638
Flexural Yield Strength 245 MPa
35600 psi
ASTM D790
Izod Impact, Notched 0.941 J/cm
1.76 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 232 °C
450 °F
ASTM D648
Flammability, UL94 V-0
V-0