Material Notes:
Information provided by Goodfellow.
Thermal Properties Metric English Comments
Melting Point 1445 °C
2633 °F
Component Elements Properties Metric English Comments
Molybdenum, Mo 16 %
16 %
Nickel, Ni 84 %
84 %