| Category | Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Unreinforced, Flame Retardant |
| Manufacturer | Cheng Yu Plastic Company Limited (formerly Luen Cheong Hong) |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Cheng Yu Plastic FR200N Flame Retardant Nylon 66.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.25 g/cc | 1.25 g/cc | ASTM D792 |
| Water Absorption | 1.0 - 2.0 % | 1.0 - 2.0 % | ASTM D570 |
| Linear Mold Shrinkage | 0.0020 - 0.020 cm/cm | 0.0020 - 0.020 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 88 | 88 | ASTM D785 |
| Tensile Strength, Yield | 73.5 MPa | 10700 psi | ASTM D638 |
| Flexural Yield Strength | 123 MPa | 17800 psi | ASTM D790 |
| Izod Impact, Notched | 0.735 J/cm | 1.38 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 220 °C | 428 °F | ASTM D648 |
| Flammability, UL94 | V-0 | V-0 |