Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lord Adhesives Thermosetâ„¢ SC-303 Silicone Encapsulant, Flame Retardant

Category Polymer , Thermoset , Silicone , Silicone, RTV, Encapsulation Grade
Manufacturer Lord Adhesives
Trade Name Thermoset™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lord Adhesives Thermosetâ„¢ SC-303 Silicone Encapsulant, Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Lord SC-303 is a two component silicone elastomer that provides excellent thermal conductivity, while retaining the other desirable properties associated with silicones. It is a low viscosity, easily pourable liquid that is ideally suited for electrical/electronic potting applications. It has excellent high heat performance, thermal shock resistance, and improved coefficient of expansion.Lord SC-303 has been formulated for flame retardancy and is an Underwriters Laboratories recognized material under the Components-Plastics classification as 94V-0 at 0. 250 inches.Lord SC-303 resin is white and the hardener is gray. These colors act as mix indicators. When thoroughly mixed, SC-303 is lighter gray.Lord SC-303 is addition curing. It will not depolymerize when heated in confined spaces as do many condensation curing silicones. As with all silicones, SC-303 generates no exotherm as it cures. It also exhibits low shrinkage and stress on components as it cures. Lord SC-303's cure may be accelerated with elevated temperature.All information provided by Lord.
Physical Properties Metric English Comments
Specific Gravity 2.10 g/cc
2.10 g/cc
STM 2
Water Absorption 0.050 %
0.050 %
ASTM D570-81
Viscosity 7000 cP

@Temperature 25.0 °C
7000 cP

@Temperature 77.0 °F
STM 1
Mechanical Properties Metric English Comments
Hardness, Shore A 45
45
ASTM D2240
Tensile Strength, Yield 1.17 MPa
170 psi
ASTM D412
Elongation at Yield 90 %
90 %
ASTM D412
Thermal Properties Metric English Comments
CTE, linear 163.33 µm/m-°C
90.739 µin/in-°F
Calculated from Volume CTE; ASTM D864
Thermal Conductivity 0.800 W/m-K
5.55 BTU-in/hr-ft²-°F
Hot Disc Transient Method
Maximum Service Temperature, Air 200 °C
392 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Flammability, UL94 V-0
V-0
0.250 inch minimum thickness
Electrical Properties Metric English Comments
Volume Resistivity 3.80e+15 ohm-cm

@Temperature 25.0 °C
3.80e+15 ohm-cm

@Temperature 77.0 °F
ASTM D257
Dielectric Constant 4.2

@Frequency 1.00e+6 Hz,
Temperature 25.0 °C
4.2

@Frequency 1.00e+6 Hz,
Temperature 77.0 °F
ASTM D150
Dielectric Strength 17.3 kV/mm
440 kV/in
ASTM D149
Dissipation Factor 0.00040

@Frequency 1.00e+6 Hz,
Temperature 25.0 °C
0.00040

@Frequency 1.00e+6 Hz,
Temperature 77.0 °F
ASTM D150
Processing Properties Metric English Comments
Cure Time 10.0 - 15.0 min

@Temperature 100 °C
0.167 - 0.250 hour

@Temperature 212 °F
25.0 - 30.0 min

@Temperature 70.0 °C
0.417 - 0.500 hour

@Temperature 158 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 50 min

@Temperature 25.0 °C
50 min

@Temperature 77.0 °F
100 grams
Shelf Life 9.00 Month

@Temperature 25.0 °C
9.00 Month

@Temperature 77.0 °F
Descriptive Properties Value Comments
Appearance Gray
Hardener
Light Gray
Mixed
White
Resin
Mix Ratio 1:1
by weight, by volume
Users viewing this material also viewed the following: