| Chem Polymer Chemlon 100 W Nylon 66, MoS2 Filled |
Nylon 66, MoS2 Filled |
Chemlon
|
| Chem Polymer Chemlon 100 X Nylon 66, Lubricated GP |
Nylon 66 |
Chemlon
|
| Chem Polymer Chemlon 102 Nylon 66, Nucleated |
Nylon 66, Nucleated |
Chemlon
|
| Chem Polymer Chemlon 109 Nylon 66, High Impact |
Nylon 66, Impact Grade |
Chemlon
|
| Chem Polymer Chemlon 109-18 G Nylon 66, 18% Glass Fiber Reinforced |
Nylon 66, 20% Glass Fiber Filled |
Chemlon
|
| Chem Polymer Chemlon 109-33 G Nylon 66, 33% Glass Fiber Reinforced |
Nylon 66, 30% Glass Fiber Filled |
Chemlon
|
| Chem Polymer Chemlon 113 G Nylon 66, 13% Glass Fiber Reinforced |
Nylon 66, 10% Glass Fiber Filled |
Chemlon
|
| Chem Polymer Chemlon 115 G Nylon 66, 15% Glass Fiber Reinforced |
Nylon 66, 20% Glass Fiber Filled |
Chemlon
|
| Chem Polymer Chemlon 125 G Nylon 66, 25% Glass Sphere Reinforced |
Nylon 66, Glass Bead Filled |
Chemlon
|
| Chem Polymer Chemlon 125-15 MG Nylon 66, 25% Mineral/15% Glass Fiber Reinforced |
Nylon 66, Glass/Mineral Filled |
Chemlon
|
| Chem Polymer Chemlon 130 GVH Nylon 66, 30% Glass Fiber Reinforced |
Nylon 66, Glass Fiber Filled, Flame Retardant |
Chemlon
|
| Chem Polymer Chemlon 133 G Nylon 66, 33% Glass Fiber Reinforced |
Nylon 66, 30% Glass Fiber Filled |
Chemlon
|
| Chem Polymer Chemlon 140 M Nylon 66, 40% Mineral Reinforced |
Nylon 66, 40% Mineral Filled |
Chemlon
|
| Chem Polymer Chemlon 143 G Nylon 66, 43% Glass Fiber Reinforced |
Nylon 66, 40% Glass Fiber Filled |
Chemlon
|
| Chem Polymer Chemlon 182 Nylon 66, Flame Retarded |
Nylon 66, Unreinforced, Flame Retardant |
Chemlon
|
| Chem Polymer Chemlon 206 G Nylon 6, 6% Glass Fiber Reinforced |
Nylon 6, 10% Glass Fiber Filled |
Chemlon
|
| Chem Polymer Chemlon 212 Nylon 6, Lubricated, GP |
Nylon 6 |
Chemlon
|
| Chem Polymer Chemlon 214 G Nylon 6, 14% Glass Fiber Reinforced |
Nylon 6, 10% Glass Fiber Filled |
Chemlon
|
| Chem Polymer Chemlon 215 GVH Nylon 6, 15% Glass Fiber Reinforced |
Nylon 6, Glass Fiber Filled, Flame Retardant |
Chemlon
|
| Chem Polymer Chemlon 217 GI Nylon 6, 17% Glass Fiber Reinforced |
Nylon 6, 20% Glass Fiber Filled |
Chemlon
|
| Chem Polymer Chemlon 218 GV Nylon 6, 18% Glass Reinforced |
Nylon 6, Glass Fiber Filled, Flame Retardant |
Chemlon
|
| Chem Polymer Chemlon 225 G Nylon 6, 25% Glass Fiber Reinforced |
Nylon 6, 30% Glass Fiber Filled |
Chemlon
|
| Chem Polymer Chemlon 225-15 MG Nylon 6, 25% Mineral/15% Glass Fiber Reinforced |
Nylon 6, Glass/Mineral Reinforced |
Chemlon
|
| Chem Polymer Chemlon 233 G Nylon 6, 33% Glass Fiber Reinforced |
Nylon 6, 30% Glass Fiber Filled |
Chemlon
|
| Chem Polymer Chemlon 233 GI Nylon 6, 33% Glass Fiber Reinforced |
Nylon 6, 30% Glass Fiber Filled |
Chemlon
|
| Chem Polymer Chemlon 233 GVH Nylon 6, 33% Glass Fiber Reinforced |
Nylon 6, Glass Fiber Filled, Flame Retardant |
Chemlon
|
| Chem Polymer Chemlon 240 G Nylon 6, 43% Glass Fiber Reinforced |
Nylon 6, 40% Glass Fiber Filled |
Chemlon
|
| Chem Polymer Chemlon 253 H Nylon 6, Impact Modified |
Nylon 6, Impact Grade |
Chemlon
|
| Chem Polymer Chemlon 256 Nylon 6, Wire Jacketing Grade |
Nylon 6, Unreinforced, Flame Retardant |
Chemlon
|
| Chem Polymer Chemlon 267 Nylon 6, Impact Modified |
Nylon 6, Impact Grade |
Chemlon
|
| Chem Polymer Chemlon 275 Nylon 6, Copolymer Impact Modified |
Nylon 6, Impact Grade |
Chemlon
|
| Chem Polymer Chemlon 282 Nylon 6, Flame Retarded |
Nylon 6, Unreinforced, Flame Retardant |
Chemlon
|
| Chem Polymer Durlex 700 PBT, General Purpose |
Polybutylene Terephthalate (PBT), Unreinforced, Molded |
Durlex
|
| Chem Polymer Durlex 709 IH PBT, Impact Modified |
Polybutylene Terephthalate (PBT), Impact Grade |
Durlex
|
| Chem Polymer Durlex 715 G PBT, 15% Glass Reinforced |
Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled |
Durlex
|
| Chem Polymer Durlex 730 G PBT, 30% Glass Fiber Reinforced |
Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled |
Durlex
|
| Chem Polymer Durlex 740 G PBT, 40% Short Glass Fiber Reinforced |
Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled |
Durlex
|
| Chem Polymer Durlex 740-10 GB PBT, 40% Short Glass Fiber, 10% Glass Bead Reinforced |
Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled |
Durlex
|
| Chem Polymer Formax 609 Acetal, Medium Flow |
Acetal Copolymer, Unreinforced |
Formax
|
| Chem Polymer Chemlon 100 Nylon 66, Lubricated GP |
Nylon 66 |
Chemlon
|
| Chem Polymer Chemlon 104 Nylon 66, Medium Impact GP |
Nylon 66, Impact Grade |
Chemlon
|
| Chem Polymer Chemlon 104-13 G Nylon 66, 13% Glass Fiber Reinforced |
Nylon 66, 10% Glass Fiber Filled |
Chemlon
|
| Chem Polymer Chemlon 223 Nylon 6, Nucleated |
Nylon 6, Nucleated |
Chemlon
|
| Chem Polymer Chemlon 280 Nylon 6, High Impact |
Nylon 6, Impact Grade |
Chemlon
|
| Chem Polymer Durlex 730 GVH PBT, 30% Glass Fiber Reinforced |
Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant |
Durlex
|
| Chem Polymer Formax 604 Acetal, Low Flow |
Acetal Copolymer, Unreinforced |
Formax
|
| Chem Polymer Formax 605 G Acetal, 5% Glass Reinforced |
Acetal Copolymer, 10% Glass Fiber Reinforced |
Formax
|
| Chem Polymer Formax 630 Acetal, High Flow |
Acetal Copolymer, Unreinforced |
Formax
|
| Chem Polymer Formax 630 G Acetal, 30% Glass Fiber Reinforced |
Acetal Copolymer, 30% Glass Fiber Reinforced |
Formax
|