Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

CMW® 353 Copper Alloy

Category Metal , Nonferrous Metal , Copper Alloy
Manufacturer CMW Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CMW® 353 Copper Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
CMW® 353 material is an economical high strength, high conductivity copper base alloy. It is a heat treatable copper base alloy and its excellent properties are obtained largely through heat treatment. Its properties combine high hardness, strength and wear resistance with relatively high electrical and thermal conductivity.CMW® 353 is superior in its combination of hardness and conductivity to such non-ferrous alloys as Yellow Brass, Gear Bronze, Manganese Bronze and Aluminum Bronze. Any current or heat conducting members in electrical or other machinery will, therefore, be improved when made of CMW® 353 material. High hardness, combined with the toughness which characterizes CMW® 353 material, gives it excellent wear resistance and makes it useful for flash welding dies, back up bars, bushings and current carrying bearings in combination with CMW®3 shafts.Information provided by CMW Inc.
Physical Properties Metric English Comments
Density 8.75 g/cc
0.316 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 90
90
Castings
Tensile Strength, Ultimate 586 MPa
85000 psi
Castings
Tensile Strength, Yield 483 MPa
70100 psi
Castings
Elongation at Break 10 %
10 %
Castings
Reduction of Area 20 %
20 %
Castings
Modulus of Elasticity 114 GPa
16500 ksi
Thermal Properties Metric English Comments
CTE, linear 16.2 µm/m-°C

@Temperature 100 °C
9.00 µin/in-°F

@Temperature 212 °F
Thermal Conductivity 183 W/m-K
1270 BTU-in/hr-ft²-°F
Melting Point 1038 - 1116 °C
1900 - 2041 °F
Solidus 1038 °C
1900 °F
Liquidus 1116 °C
2041 °F
Softening Point 455 °C
851 °F
Permanent Softening
Component Elements Properties Metric English Comments
Chromium, Cr 0.80 %
0.80 %
Copper, Cu 96.1 %
96.1 %
Nickel, Ni 2.5 %
2.5 %
Silicon, Si 0.60 %
0.60 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000359 ohm-cm
0.00000359 ohm-cm
48 % IACS
Users viewing this material also viewed the following: