Dandong Taico Minerals TAICOCITE® TC3 Magnesium Hydroxide

Category Ceramic
Manufacturer Dandong Taico Minerals
Trade Name TAICOCITE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dandong Taico Minerals TAICOCITE® TC3 Magnesium Hydroxide.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Made from local natural brucite minerals, TAICOCITE® is the name of milled magnesium hydroxide products which is produced (micronized/surface treated) by Dandong Taico Minerals Co., Ltd. TAICOCITE® magnesium hydroxides are effective flame retardant fillers for polymeric materials, achieving high values of limiting oxygen index, smoke emission reduction and toxic gas absorption. TAICOCITE® flame retardants are odorless, non-toxic, white micronized powder of normal size distribution. According to requirements from different customers, we provide TAICOCITE® flame retardants with different size distributions, specific surface area and surface modifications to bring the final products different properties; The surface modifications could bring following properties: Improves compatibility and dispersion uniformity, Enhances flame retardant performance, Improves physical properties, Less equipment abrasion and Higher throughput ratesInformation provided by Dandong Taico Minerals
Physical Properties Metric English Comments
Density 2.30 g/cc
0.0831 lb/in³
Brightness 90 %
90 %
Whiteness
Oil Absorption 50 - 55 %
50 - 55 %
ml/100g
Loss On Ignition 30 - 34 %
30 - 34 %
Particle Size 15 µm
15 µm
D50
40 µm
40 µm
D90
pH 9.0 - 10
9.0 - 10
Specific Surface Area 6.0 - 8.0 m²/g
6.0 - 8.0 m²/g
Thermal Properties Metric English Comments
Decomposition Temperature 330 - 340 °C
626 - 644 °F
Optical Properties Metric English Comments
Refractive Index 1.561 - 1.581
1.561 - 1.581
Component Elements Properties Metric English Comments
CaO <= 1.0 %
<= 1.0 %
Fe2O3 <= 0.50 %
<= 0.50 %
Free Water <= 0.50 %
<= 0.50 %
SiO2 <= 3.0 %
<= 3.0 %
Descriptive Properties Value Comments
Acid insoluble <2%
Activation Index >95%
Mg(OH)2 >94%