| Category | Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), UHMW PE Ultra High Molecular Weight |
| Manufacturer | Quadrant Engineering Plastics Products |
| Trade Name | TIVAR® |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Quadrant EPP Tivar® Premium UHMW-PE Tivar Premium UHMW-PE.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 0.930 g/cc | 0.930 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength | 4200 MPa | 609000 psi | ASTM D638 |
| Elongation at Break | 158 % | 158 % | ASTM D638 |
| Tensile Modulus | 0.896 GPa | 130 ksi | ASTM D638 |
| Flexural Strength | 22.1 MPa | 3200 psi | ASTM D790 |
| Flexural Modulus | 0.745 GPa | 108 ksi | ASTM D790 |
| Compressive Strength | 20.7 MPa @Strain 10.0 %, Temperature 22.8 °C |
3000 psi @Strain 10.0 %, Temperature 73.0 °F |
ASTM D695 |
| Compressive Modulus | 0.552 GPa | 80.0 ksi | ASTM D695 |
| Coefficient of Friction, Dynamic | 0.15 | 0.15 | DRY VS STEEL; QTM 55007 |
| Sand Slurry | 9.0 | 9.0 | 1018 STEEL = 100; ASTM D4020 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 135 °C | 275 °F | CRYSTALLINE; ASTM D3418 |