Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ashley Polymers Ashlene® 538 Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Extruded
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® 538 Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
A general purpose high viscosity extrusion grade Nylon 66.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ASTM D792
Water Absorption 1.2 %
1.2 %
24 hrs; ASTM D570
Water Absorption at Saturation 8.5 %
8.5 %
ASTM D570
Linear Mold Shrinkage 0.0125 cm/cm
0.0125 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength, Yield 85.0 MPa
12300 psi
ASTM D638
Elongation at Break 90 %
90 %
ASTM D638
Flexural Modulus 3.00 GPa
435 ksi
ASTM D790
Izod Impact, Notched 0.640 J/cm
1.20 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 254 °C
489 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 100 °C
212 °F
ASTM D648
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
Dielectric Constant 3.5

@Frequency 1e+6 Hz
3.5

@Frequency 1e+6 Hz
ASTM D150
Users viewing this material also viewed the following: