Material Notes:
A general purpose, injection molding grade, natural resin.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ASTM D792
Water Absorption 0.15 %
0.15 %
ASTM D570
Moisture Absorption at Equilibrium 0.34 %
0.34 %
ASTM D570
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
ASTM D955
Melt Flow 10 g/10 min
10 g/10 min
Cond. 300/1.2
Mechanical Properties Metric English Comments
Hardness, Rockwell M 70
70
ASTM D785
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength, Ultimate 66.0 MPa
9570 psi
ATSM D638
Elongation at Break 125 %
125 %
ASTM D638
Elongation at Yield 6.0 %
6.0 %
ASTM D638
Flexural Modulus 2.20 GPa
319 ksi
ASTM D790
Compressive Yield Strength 76.0 MPa
11000 psi
ASTM D695
Izod Impact, Notched 8.54 J/cm
16.0 ft-lb/in
ASTM D256
Tensile Impact Strength 580 kJ/m²

@Thickness 3.20 mm
276 ft-lb/in²

@Thickness 0.126 in
ASTM D1822S
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 132 °C
270 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 125 °C
257 °F
ASTM D648