| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.913 g/cc | 0.0330 lb/in³ | |
| Melt Flow | 30 g/10 min @Load 2.16 kg |
30 g/10 min @Load 4.76 lb |
Melt flow ratio I10/I2 is 7. |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 96 | 96 | |
| Tensile Strength, Yield | 8.30 MPa | 1200 psi | |
| Elongation at Break | 700 % | 700 % | |
| Modulus of Elasticity | 0.178 GPa | 25.8 ksi | Molded Sample 2% Secant Modulus |
| Flexural Modulus | 0.239 GPa | 34.7 ksi |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Vicat Softening Point | 88.0 °C | 190 °F |